Shield grouting material, preparation method thereof and intelligent preparation device of shield grouting material
A grouting material and shield technology, applied in the field of shield grouting materials, can solve problems such as manpower and time consumption, raw material dosage errors, etc., to improve mixing efficiency, increase overall performance, and ensure overall use experience and work efficiency. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Embodiment 1: a shield grouting material configuration method, comprising the following steps:
[0037] Raw material preparation: Prepare the raw materials required for grouting materials; the raw materials include: 300 parts of water, 50 parts of cement, 300 parts of fly ash, 50 parts of bentonite, 700 parts of sand, 50 parts of titanate, polymer micro 25 parts of beads, 40 parts of composite filler, 50 parts of iron oxide, 20 parts of glass powder and ground glass fiber filler, 15 parts of ethylene glycol, 10 parts of air-entraining agent, 20 parts of stabilizer, 25 parts of waterproofing agent, water reducing agent 10 parts of plasticizer, 35 parts of plasticizer, and 20 parts of expansion agent; the fly ash is superfine fly ash; the bentonite is nanobase pulping bentonite; the sand is quartz sand; the titanate is transition metal Titanate, the titanate is used to improve the acid and alkali resistance of the grouting material; the polymer microbeads are polymer vitr...
Embodiment 2
[0043] Embodiment 2: a shield grouting material configuration method, comprising the following steps:
[0044]Raw material preparation: Prepare the raw materials required for grouting materials; the raw materials include: 340 parts of water, 100 parts of cement, 350 parts of fly ash, 80 parts of bentonite, 720 parts of sand, 60 parts of titanate, polymer micro 30 parts of beads, 45 parts of composite filler, 60 parts of iron oxide, 30 parts of glass powder and ground glass fiber filler, 20 parts of ethylene glycol, 20 parts of air-entraining agent, 30 parts of stabilizer, 30 parts of waterproofing agent, water reducing agent 20 parts of agent, 40 parts of plasticizer, and 25 parts of expansion agent; the fly ash adopts ultra-fine fly ash; the bentonite adopts nanobase pulping bentonite; the sand adopts quartz sand; the titanate adopts transition metal Titanate, the titanate is used to improve the acid and alkali resistance of the grouting material; the polymer microbeads are p...
Embodiment 3
[0049] Embodiment 3: comprise the following steps:
[0050] Raw material preparation: Prepare the raw materials required for grouting materials; the raw materials include: 400 parts of water, 150 parts of cement, 400 parts of fly ash, 100 parts of bentonite, 750 parts of sand, 70 parts of titanate, polymer micro 35 parts of beads, 55 parts of composite filler, 65 parts of iron oxide, 35 parts of glass powder and ground glass fiber filler, 25 parts of ethylene glycol, 25 parts of air-entraining agent, 35 parts of stabilizer, 45 parts of waterproofing agent, water reducing agent 30 parts of agent, 65 parts of plasticizer, and 30 parts of expansion agent; the fly ash adopts ultra-fine fly ash; the bentonite adopts nanobase pulping bentonite; the sand adopts quartz sand; the titanate adopts transition metal Titanate, the titanate is used to improve the acid and alkali resistance of the grouting material; the polymer microbeads are polymer vitrified microbeads, and the polymer micr...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com