Inorganic mineral interior wall coating and preparation method thereof
A technology of interior wall paint and inorganic minerals, applied in the direction of coating, etc., to achieve the effect of reducing carbon emissions and environmental protection of living space
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Example 1: Cellulose and / or polysaccharides
[0033] A preparation method of inorganic mineral interior wall paint, the method comprises the steps of:
[0034] Select 1 gram of stearic acid, 1 gram of water glass, 1 gram of polydimethylsiloxane, 150 grams of natural mineral pigments (50 grams of titanium dioxide and 100 grams of kaolin) and 150 grams of natural mineral fillers (83 grams of wollastonite powder) according to the corresponding proportions. , 55.5 grams of heavy calcium and 111.5 grams of talcum powder) 250 grams, 350 grams of modified potassium silicate, 2 grams of cellulose and 245 grams of water are mixed to obtain a liquid finished product.
Embodiment 2
[0036] A preparation method of inorganic mineral interior wall paint, the method comprises the steps of:
[0037] Select 1 gram of sodium dodecylbenzene sulfonate, 1 gram of sodium tripolyphosphate, 1 gram of alkyne alcohol, 180 grams of natural mineral pigment (60 grams of titanium dioxide and 120 grams of kaolin), 180 grams of natural mineral filler (wollastonite powder) according to the corresponding proportions. 86 grams, 64 grams of heavy calcium and 150 grams of talcum powder) 300 grams, 350 grams of modified potassium silicate, 2 grams of polysaccharides and 165 grams of water are mixed to obtain a liquid finished product.
Embodiment 3
[0039] A preparation method of inorganic mineral interior wall paint, the method comprises the steps of:
[0040] Select 1.2 grams of quaternary ammonium compounds, 1.5 grams of sodium hexametaphosphate, 1 gram of polydimethylsiloxane, 200 grams of natural mineral pigments (60 grams of titanium dioxide and 140 grams of kaolin) and 200 grams of natural mineral fillers (diatomaceous earth) according to the corresponding proportions. 42 grams, 62 grams of heavy calcium and 146 grams of talcum powder) 250 grams, 380 grams of modified potassium silicate, 3 grams of cellulose and 163.3 grams of water are mixed to obtain a liquid finished product.