Zinc oxide flotation recovery method based on combination of gravity and flotation selection and pre-desliming
A recovery method, zinc oxide technology, applied in chemical instruments and methods, flotation, mechanical material recovery, etc., can solve problems such as large number of desliming tanks, poor foam outflow, excessive foam volume, etc., and achieve high efficiency and stability The effect of removal
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0054] Embodiment 1 provides a kind of zinc oxide flotation recovery method based on refloating joint desliming in advance, comprises the following steps:
[0055] S1. Pretreat the zinc oxide ore to be selected to obtain ore powder, mix the ore powder and water to obtain a primary slurry; the mass fraction of the ore powder in the primary slurry is 36%; the solid particles with a particle size of less than 0.074mm in the primary slurry account for the ore powder 69% of the total mass;
[0056] S2. Carrying out the zinc sulfide flotation process of once roughing, twice sweeping, and twice selected zinc sulfide flotation process on the primary pulp obtained in step S1, to obtain zinc sulfide concentrate and zinc sulfide tailings, specifically comprising the following steps:
[0057] S21. Add sulfur 250g / t copper acid copper, 50g / t butyl sodium xanthate, and 17g / t pinitol to the primary pulp, and perform zinc sulfide roughing for 3 minutes to obtain zinc sulfide roughing concentr...
Embodiment 2
[0079] Embodiment 2 provides a zinc oxide flotation recovery method based on heavy flotation combined with desliming in advance. Compared with Example 1, the difference is that the dosage of chemicals in each step is adjusted. The specific adjustments are as follows, and the rest are the same as those in the implementation Example 1 is roughly the same, and will not be repeated here.
[0080] In step S2, 200g / t of copper sulfate, 40g / t of butyl sodium xanthate and 15g / t of terpineol oil are used for zinc sulfide roughing agent, 20g / t of butyl sodium xanthate for the first zinc sulfide sweeping agent, and 20g / t of butyl sodium xanthate for the first time. Secondary zinc sulfide sweep agent butyl sodium xanthate 10g / t, first zinc sulfide selective agent water glass 200g / t;
[0081] In step S4, the flotation desliming agent is 50 g / t of butyl sodium xanthate, and 50 g / t of Lp-1 agent;
[0082] In step S5, zinc oxide first roughing agent sodium carbonate 3000g / t, water glass 2500...
Embodiment 3
[0087] Embodiment 3 provides a zinc oxide flotation recovery method based on heavy flotation combined with desliming in advance. Compared with Embodiment 1, the difference is that the mass percentage of ore powder in the primary slurry in step S1 is adjusted and is less than 0.074mm The mass percentage of mineral powder, the concentration of secondary pulp in step S4, and the dosage of chemicals in each step are specifically adjusted as follows, and the rest are roughly the same as in Example 1, and will not be repeated here.
[0088] In step S1, the mass percentage of ore powder in the primary slurry is not more than 33%, and the mass percentage of ore powder less than 0.074mm is 71%;
[0089] In step S2, copper sulfate 300g / t, butyl sodium xanthate 60g / t and terpineol oil 20g / t are used for zinc sulfide roughing agent, butyl sodium xanthate 30g / t for the first zinc sulfide sweeping agent, and butyl sodium xanthate 30g / t for the first time. Secondary zinc sulfide sweep agent ...
PUM