Antistatic soft wool fabric and preparation method thereof
An antistatic and wool technology, applied in the direction of textile, animal fiber, yarn, etc., can solve the problems of non-soft fabrics, inflammation, static electricity, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A method for preparing an antistatic soft wool fabric, the preparation method of the antistatic soft wool fabric mainly includes the following preparation steps:
[0032] (1) primary twisting: the wool fiber is twisted to 30D by a twisting machine to obtain primary spinning;
[0033] (2) Bacteria treatment: immerse the primary spinning thread in a solution blended with sodium nitrate, dipotassium hydrogen phosphate, magnesium sulfate, potassium chloride, ferrous sulfate and distilled water at a mass ratio of 3:1:0.5:0.5:0.01:1000 , and then add a bacterial solution of 0.5 times the quality of the spinning thread, and let it stand for 40 hours under the condition of a sealed tank at 37°C;
[0034] (3) Enzyme treatment: after the streptomyces treatment is completed, open the sealed sealed tank, add muramidase of 0.01 times the mass of the primary spinning line and phospholipase of 0.01 times the mass of the primary spinning line, at 37°C at a speed of 100r / min Stir for 3...
Embodiment 2
[0047] A method for preparing an antistatic soft wool fabric, the preparation method of the antistatic soft wool fabric mainly includes the following preparation steps:
[0048] (1) Bacteria treatment: immerse the wool fiber in a solution blended with sodium nitrate, dipotassium hydrogen phosphate, magnesium sulfate, potassium chloride, ferrous sulfate and distilled water at a mass ratio of 3:1:0.5:0.5:0.01:1000, Then add the bacterial solution of 0.5 times the wool fiber mass, and let it stand for 40 hours under the condition of sealing the sealed tank at 37°C;
[0049] (2) Enzyme treatment: After the streptomyces treatment is completed, open the sealed sealing tank, add muramidase with 0.01 times the mass of wool fiber and phospholipase with 0.01 times the mass of wool fiber, and stir at 37°C at a speed of 100r / min for 3min After standing still for 6 hours, the wool fibers were taken out and immersed in deionized water at 20°C for 3 minutes, and dried at 60°C for 8 hours to ...
Embodiment 3
[0062] A method for preparing an antistatic soft wool fabric, the preparation method of the antistatic soft wool fabric mainly includes the following preparation steps:
[0063] (1) primary twisting: the wool fiber is twisted to 30D by a twisting machine to obtain primary spinning;
[0064] (2) Bacteria treatment: immerse the primary spinning thread in a solution blended with sodium nitrate, dipotassium hydrogen phosphate, magnesium sulfate, potassium chloride, ferrous sulfate and distilled water at a mass ratio of 3:1:0.5:0.5:0.01:1000 , and then add a bacterial solution of 0.5 times the quality of the spinning thread, and let it stand for 40 hours under the condition of a sealed tank at 37°C;
[0065] (3) Secondary twisting: Twisting the primary spinning twister after bacterial treatment to 90D to obtain secondary spinning;
[0066] (4) Hollow cell wall immobilization treatment: immerse the secondary spinning thread in a sodium hydroxide solution with a mass fraction of 10%...
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com