Embodiment 1
[0020] Prepare 1000kg compound mineral type ruminant licking brick.
[0021] A: Take 3000g of copper sulfate, 7000g of zinc sulfate, 650g of cobalt chloride, 800g of potassium iodide, 750g of sodium selenite, and 200kg of calcium hydrogen phosphate, and mix the above materials with 300kg of whole wheat flour and stir evenly.
[0022] B: Take 250kg of table salt, 50kg of red clay, 50kg of calcium oxide, and 138kg of sodium bentonite, and add them into the mixture obtained in A process and stir.
[0023] C: Atomize 75kg of drinking water and spray it into the mixture obtained in the process of B. Stir evenly and press it into 500 pieces according to the weight of 2kg per piece.
Embodiment 2
[0025] A: Take 4500g of copper sulfate, 10500g of zinc sulfate, 975g of cobalt chloride, 1200g of potassium iodide, 1125g of sodium selenite, and 200kg of calcium hydrogen phosphate, and mix the above materials with 300kg of whole wheat flour and stir evenly.
[0026] B: Take 250kg of table salt, 50kg of red gum clay, 50kg of calcium oxide, and 132kg of sodium bentonite, and add them into the mixture obtained in A process and stir.
[0027] C: Atomize 75kg of drinking water and spray it into the mixture obtained in the process of B. Stir evenly and press it into 500 pieces according to the weight of 2kg per piece.
Embodiment 3
[0029] A: Take 4000g of copper sulfate, 9500g of zinc sulfate, 975g of cobalt chloride, 1000g of potassium iodide, 950g of sodium selenite, and 200kg of calcium hydrogen phosphate, mix the above materials with 300kg of whole wheat flour and stir evenly.
[0030] B: Take 250kg of table salt, 50kg of red gum clay, 50kg of calcium oxide, and 132kg of sodium bentonite, and add them into the mixture obtained in A process and stir.
[0031] C: Atomize 75kg of drinking water and spray it into the mixture obtained in the process of B. Stir evenly and press it into 500 pieces according to the weight of 2kg per piece.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com