Problems solved by technology

[0020] The cationically modified cellulose derivative forms a complex salt with an anionic surfactant when preparing a hair treatment composition and adsorbs on the hair, and exhibits an excellent conditioning effect when washed, whereas it exhibits an excellent conditioning effect after drying. Hard feeling, there is a problem that the tactile feeling deteriorates
In addition, although cationic modified guar gum has little hard feeling after drying, the adsorption capacity is small, and there is a problem of poor conditioning effect during washing.
In addition, due to the diversification of styles in recent years, the use of hair colorants and hair dyes has increased, and the accompanying damage to the hair has been significant. Even cationic modified guar gum and cationic modified locust bean gum have Insufficient softness to damaged hair, showing problems with hair stiffness
In addition, when blending conditioners such as cationic polymers and moisturizing agents such as glycerin into skin cosmetic compositions, stickiness and stickiness may sometimes occur depending on the blending amount in the formulation.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Cation-modified galactomannan polysaccharide and cosmetic composition containing the same
  • Cation-modified galactomannan polysaccharide and cosmetic composition containing the same
  • Cation-modified galactomannan polysaccharide and cosmetic composition containing the same

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0071] After adding 11.8 g of 48 mass % sodium hydroxide aqueous solution and 3.0 g of sodium chloride to 900 ml of 80 volume % isopropanol aqueous solution, slowly add and disperse fenugreek gum (fenugreek endosperm powder A, Ea- Green Co., Ltd.) 162 g. Next, 40.5 g of an aqueous solution of 80% by mass glycidyltrimethylammonium chloride (hereinafter also referred to as GTA) was added, heated, and reacted at 50° C. for 3 hours. After completion of the reaction, 14.0 g of 35% hydrochloric acid was diluted with 1500 ml of 70% by volume isopropanol aqueous solution for neutralization. After neutralizing at room temperature for 1 hour, the reaction liquid was poured into 800 ml of methanol, and the reaction product was precipitated and filtered. After the obtained precipitate was washed with methanol aqueous solution, the reaction product was dried under reduced pressure. The cationic charge of the cationically modified galactomannan thus obtained was 0.75 meq / g. The results a...

Embodiment 2

[0074] Disperse 162 g of fenugreek gum (Fenugreek endosperm powder A, manufactured by Air Glynn Co., Ltd.) in 900 ml of 55% by volume isopropanol aqueous solution, and add 6.0 g of sodium chloride and 48% by mass of hydrogen Sodium oxide aqueous solution 48.9g. Then, 152.3 g of 3-halo-2-hydroxypropyldimethylmonolauryl ammonium chloride was added, heated, and reacted at 50° C. for 3 hours. After completion of the reaction, 14.0 g of 35% hydrochloric acid was diluted with 1500 ml of 70% by volume isopropanol aqueous solution for neutralization. After neutralizing at room temperature for 1 hour, the reaction liquid was poured into 800 ml of methanol, and the reaction product was precipitated and filtered. After the obtained precipitate was washed with methanol aqueous solution, the reaction product was dried under reduced pressure. The cationic charge of the cationically modified galactomannan thus obtained was 0.80 meq / g. The results are shown in Table 1 (Sample No. 4 in Tabl...

Embodiment 3

[0076] Disperse 162 g of fenugreek gum (Fenugreek endosperm powder A, manufactured by Air Glynn Co., Ltd.) in 900 ml of 80% by volume isopropanol aqueous solution in a pressurized airtight container, and add 48% by mass of hydrogen Sodium oxide aqueous solution 11.8g. Then, 66 g of ethylene oxide and 240 g of propylene oxide were added, heated, and pressurized sealing reaction was carried out at 70° C. for 3 hours. After the reaction was completed, the pressure was released and cooled to 50°C. After cooling, 150 g of an 80% by mass GTA aqueous solution was added and reacted at 50° C. for 3 hours. After completion of the reaction, 14.0 g of 35% hydrochloric acid was diluted with 1500 ml of 70% by volume isopropanol aqueous solution for neutralization. After neutralizing at room temperature for 1 hour, the reaction liquid was poured into 800 ml of methanol, and the reaction product was precipitated and filtered. After the obtained precipitate was washed with methanol aqueous ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The present invention provides a cation-modified galactomannan polysaccharide which gives excellent conditioning effects and gives good feeling and flexibility when it is used in a hair treatment compostion, and improves feeling of use by conditioning effects and emulsification conditions when it is used in a skin cosmetic composition such as body cleansing agent. Concretely, the present invention provides a cation-modified galactomannan polysaccharide obtained by substituting some of hydroxyl groups contained in an cation-modified galactomannan polysaccharide which is nonionic polysaccharideand constitutes mannose as a main chain and galactose as a side chain and the composition ratio of mannose and galactose is 1:1 and obtained from albumen portion of a seed of fenugreek (Trigonella foenum-graecum) which is a leguminus plant, with a specific quaternary nitrogen-containing group, and a cosmetic composition containing the cation-modified galactomannan.

Description

[0001] This divisional application is based on the application number 200480010882.4 (international application number: PCT / JP2004 / 006512), the application date is May 07, 2004, and the invention name is "cationically modified galactomannan and cosmetics containing it". The divisional application of the Chinese patent application of "Material Composition". technical field [0002] The present invention relates to a cation-modified galactomannan and a cosmetic composition containing the same, especially a hair treatment composition, when the cation-modified galactomannan is formulated into the cosmetic composition At the same time, it has good adsorption to hair and skin, which can bring good conditioning effect, and because of its emulsifying property, it can bring a good finishing feeling without a stiff feeling after drying. technical background [0003] In order to improve the damage caused by hair tangling during shampooing and rinsing and the feeling after shampooing, c...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): A61K8/73A61K8/84A61K8/89A61Q5/12A61Q1/00A61Q19/10C08B37/00
CPCA61Q1/00A61K2800/5426A61K8/737A61Q19/10C08B37/0087A61Q5/12A61K8/9789
Inventor 武田博光森芳彦
Owner TOHO CHEM IND