A technology of lufenuron and water emulsion, applied in the field of pesticides and their preparation, can solve problems such as lax management, phytotoxicity, environmental pollution, etc., and achieve obvious effects of social benefits, promotion of environmental protection, and obvious economic benefits
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0036] Raw material formula: Lufenuron technical 3kg, solvent xylene 2kg, emulsifier polyoxyethylene alkylphenol 1.5kg, thickener polyvinyl alcohol or xanthan gum 1.8kg, antifreeze agent ethylene glycol or propylene glycol 1.6kg, disinfectant Foaming agent silicone 0.2kg, water 89.9kg.
[0037] Preparation method: according to the above formula, pour lufenuron into the organic solvent xylene or toluene, stir continuously until lufenuron is completely dissolved, and use it as the oil phase for later use;
[0038] Add the emulsifier, thickener, antifreeze, and defoamer to the water under stirring according to the above formula, and keep stirring until it completely dissolves into a uniform liquid, and use it as the water phase for later use.
[0039] First add the oil phase to the container of the shearing machine, start stirring, then gradually add the water phase to the oil phase under stirring, control the speed at 1000 rpm, stir for 60 minutes, and it will become a milky whi...
Embodiment 2
[0041] Raw material formula
[0042] Lufenuron technical 10kg, solvent xylene or toluene 5kg, emulsifier polyoxyethylene fatty alcohol 3.6kg thickener polyoxyethylene alcohol or xanthan gum 3.5kg, antifreeze agent ethylene glycol or propylene glycol 2kg, defoamer organic Silicon 0.3kg, water 75.6kg.
[0043] Preparation method: according to the above formula, add lufenuron technical into the organic solvent xylene or toluene, stir continuously until the lufenuron technical is completely dissolved, and use it as the oil phase for later use;
[0044] Add the emulsifier, thickener, antifreeze, and defoamer to the water under stirring according to the above formula, and keep stirring until it completely dissolves into a uniform liquid, and use it as the water phase for later use;
[0045] First add the oil phase to the container of the shearing machine, start stirring, then gradually add the water phase to the oil phase under stirring, control the speed at 12000 rpm, stir for 30 ...
Embodiment 3
[0047] Raw material formula:
[0048] Lufenuron technical 16KG, solvent xylene and toluene mixture 8KG, emulsifier polyoxyethylene alkylaryl phenol and sorbitol ester mixture 8kg, thickener polyvinyl alcohol or xanthan gum 4kg, antifreeze ethylene glycol The mixture of alcohol and propylene glycol is 4kg, the antifoaming agent silicone is 0.8kg, and water is 59.2kg.
[0049] Preparation method: according to the above formula, add lufenuron technical substance into the mixture of organic solvent xylene and toluene, stir continuously until lufenuron is completely dissolved, and use it as the oil phase for later use.
[0050] Then according to the above formula, add the dimehypo technical, emulsifier, thickener, antifreeze, and defoamer into the water sequentially under stirring, and keep stirring until it completely dissolves into a uniform liquid, and use it as the water phase for later use.
[0051] First add the oil phase to the container of the shearing machine, start stirr...