Water-based wax cleaning agent
A wax remover and water-based technology, applied in the field of water-based wax remover, can solve problems such as poor fluidity, and achieve the effect of improving poor fluidity, good wax removal effect, and low-carbon and environmentally friendly raw materials
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Active ingredient composition (weight percent)
[0023] Polyoxypropylene propylene glycol ether 3%, Tween-802%, wax crystal dispersant 2%, sodium hydroxide 1%, antifreeze 5%, ethanol 2%, and the rest is tap water.
[0024] Wax crystal dispersant: acrylate, styrene and maleic anhydride in a weight ratio of 9:1:1.
[0025] Antifreeze (weight ratio): 70% propylene glycol butyl ether, 20% ethanol, 10% ethylene glycol butyl ether acetate.
[0026] The preparation method is as follows: mix the polyether-type nonionic surfactant, Tween-80, and tap water according to the proportion, stir at a speed of 300-400r / min at room temperature, and stir for 15-30min, and then follow the proportion according to the proportion Add sodium hydroxide, wax crystal dispersant, antifreeze, and ethanol, and stir at a speed of 300-400r / min respectively, and the stirring time is 10-15min.
Embodiment 2
[0028] Polyoxypropylene propylene glycol ether 5%, Tween-804%, wax crystal dispersant 4%, sodium hydroxide 2%, antifreeze 5%, ethanol 4%, and the rest is tap water.
[0029] Wax crystal dispersant: acrylate, styrene and maleic anhydride in a weight ratio of 9:1:1.
[0030] Antifreeze (weight ratio): 70% propylene glycol butyl ether, 20% ethanol, 10% ethylene glycol butyl ether acetate.
[0031] The preparation method is as follows: mix the polyether-type nonionic surfactant, Tween-80, and tap water according to the proportion, stir at a speed of 300-400r / min at room temperature, and stir for 15-30min, and then follow the proportion according to the proportion Add sodium hydroxide, wax crystal dispersant, antifreeze, and ethanol, and stir at a speed of 300-400r / min respectively, and the stirring time is 10-15min.
Embodiment 3
[0033] 10% polyoxypropylene propylene glycol ether, Tween-807%, 6% wax crystal dispersant, 3% sodium hydroxide, 5% antifreeze, 8% ethanol, and the rest is tap water.
[0034] Wax crystal dispersant: acrylate, styrene and maleic anhydride in a weight ratio of 9:1:1.
[0035] Antifreeze (weight ratio): 70% propylene glycol butyl ether, 20% ethanol, 10% ethylene glycol butyl ether acetate.
[0036] The preparation method is as follows: mix the polyether-type nonionic surfactant, Tween-80, and tap water according to the proportion, stir at a speed of 300-400r / min at room temperature, and stir for 15-30min, and then follow the proportion according to the proportion Add strong sodium oxide, wax crystal dispersant, antifreeze, and ethanol, and stir at a speed of 300-400r / min, and the stirring time is 10-15min.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com