Embodiment 1
[0025] Yarn selection: 30 lbs of blended yarn of 30% kapok fiber and 70% soft silk protein regenerated fiber is selected as the warp yarn, and 21 lbs of blended yarn of 30% kapok fiber and 70% soft silk protein regenerated fiber are selected count as weft yarn. The kapok fiber has low density, good moisture absorption and moisture conductivity, soft hand feeling, warm and smooth touch, but the kapok fiber is short in length, low in strength and poor in cohesion. Soft silk protein fiber not only has the advantages of bright and soft luster, good moisture absorption and release, good fiber softness, and good fabric drapability, but also has health care functions such as absorbing ultraviolet rays, far infrared rays, and negative oxygen ions. Soft silk fiber has long length and good uniformity, and can be blended with kapok fiber to complement each other. It is a green and environmentally friendly fiber yarn.
[0026] Weaving: For the blended yarn of kapok fiber and soft silk pr...
Embodiment 2
[0038] Select the yarn: select Tencel G1001 of 40 British counts as the warp yarn, and 40 British counts of the blended yarn of 70% wool and 30% Tencel G100 as the weft yarn. Tencel has the comfort of natural fibers, and its strength is close to that of polyester, which is the highest strength among all recycled fibers. Tencel and wool fibers complement each other, which can improve spinnability, and the product is elastic, smooth and waxy to the touch, and has a solid body. Weaving: the warp and weft yarns adopt a three-up and one-down twill weave, and the warp and weft interweaving density is 133×72 / inch, and the gray cloth is obtained on a rapier loom.
[0039] Scouring: High-efficiency scouring agent TF-1884 (Transfar Chemical Industry) 8g / L, treatment temperature 95°C, holding time 60min, then wash with water.
[0040] Bleaching: 6g / L hydrogen peroxide (35%), 3g / L sodium hydroxide, 0.5g / L oxygen bleaching stabilizer (Transfar Chemical Industry), the initial setting is 50...
Embodiment 3
[0050] Select the yarn: select Tencel G1001 of 40 British counts as the warp yarn, and 40 British counts of the blended yarn of 70% wool and 30% Tencel G100 as the weft yarn. Tencel has the comfort of natural fibers, and its strength is close to that of polyester, which is the highest strength among all recycled fibers. Tencel and wool fibers complement each other, which can improve spinnability, and the product is elastic, smooth and waxy to the touch, and has a solid body. Weaving: the warp and weft yarns adopt a three-up and one-down twill weave, and the warp and weft interweaving density is 133×72 / inch, and the gray cloth is obtained on a rapier loom.
[0051] Scouring: High-efficiency scouring agent TF-1884 (Transfar Chemical Industry) 8g / L, treatment temperature 95°C, holding time 60min, then wash with water.
[0052] Bleaching: 6g / L hydrogen peroxide (35%), 3g / L sodium hydroxide, 0.5g / L oxygen bleaching stabilizer (Transfar Chemical Industry), the initial setting is 50...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com