An ultra-fine fiber, composite thermal insulation technology, applied in the field of building wall thermal insulation boards, can solve the problems of small heat storage coefficient, can not meet the requirements of specifications, high temperature resistance, etc., and achieve strong deformation adaptability and excellent impact resistance. , to ensure the effect of stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Mix 6.5kg of slag with 1.5kg of soda ash and 2kg of borax as raw materials. After pre-pressing and molding into block-shaped raw materials, they are put into a resistance furnace for melting, and the molten slag liquid flows out in a trickle, and then centrifuged Roller throwing and high-pressure energy-carrying gas make the melt into very fine gray-white fibers, which are slag superfine fibers, with a diameter of about 4 microns.
Embodiment 2
[0027] Put 4kg of water in the beater, press microsilica fume, fumed silica (model: fumed silica HL-150, Shandong Hongxiang Zinc Industry Co., Ltd.), AES resin (model: Japan TECHNOW220, Dongguan City Runxiang Plastic Raw Materials Co., Ltd.), the sequential feeding of slag microfibers and skeleton microfibers prepared in Example 1, wherein slag superfine fibers 550g, skeleton superfine fibers 150g, microsilica fume 150g, fumed silica 50g, 100g AES resin, stirred at 3000 rpm for 10 minutes to make a uniform slurry with a concentration of 9%, put the prepared plastic slurry into the mold, and then vacuum filter to obtain a plate-shaped Or massive microfiber composite molded thermal insulation board 1 .
Embodiment 3
[0029] The water of 4kg is put in the beater, feeds in the order of microsilica fume, fumed silica, AES resin, slag ultrafine fiber, skeleton ultrafine fiber, wherein the slag ultrafine fiber 600g that embodiment 1 prepares, skeleton Microfiber 100g, microsilica fume 160g, fumed silica 40g, AES resin 100g, stirred for 10 minutes at a speed of 3000 rpm, and made a uniform concentration of 8% slurry, the prepared plastic slurry The material is fed into the mold, and then vacuum filtered to obtain a plate-shaped or block-shaped superfine fiber composite molding thermal insulation board 2 .
PUM
| Property | Measurement | Unit |
|---|---|---|