[0008] A durable marking paint made from the following raw materials in parts by weight:
[0009] 6 parts of alkyd resin, 3 parts of graphene, 5 parts of ethyl acetate, 2 parts of aluminum oxide, 4 parts of amino resin, 8 parts of sepiolite powder, 5 parts of isobutyl alcohol, 3 parts of ethylene glycol, 1 part of plasticizer, 2 parts of copper alloy powder, 4.5 parts of alcohol-soluble resin, 3 parts of stearic acid, 2 parts of calcium carbonate, 1 part of bougainvillea sawdust, 6 parts of chlorinated paraffin, 1 part of barium sulfate, and 2 parts of fluorescent powder.
Embodiment 2
[0011] A durable marking paint made from the following raw materials in parts by weight:
[0012] 9 parts of alkyd resin, 6 parts of graphene, 8 parts of ethyl acetate, 4 parts of aluminum oxide, 7 parts of amino resin, 11 parts of sepiolite powder, 7 parts of isobutyl alcohol, 5 parts of ethylene glycol, 3 parts of plasticizer, 4 parts of copper alloy powder, 8 parts of alcohol-soluble resin, 7 parts of octadecyl stearic acid, 5 parts of calcium carbonate, 5 parts of bougainvillea sawdust, 14 parts of chlorinated paraffin, 2 parts of barium sulfate, and 5 parts of fluorescent powder.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com