Clothianidin sustained-release granule and preparation method thereof
A technology of clothianidin and slow-release type, which is applied in the field of clothianidin slow-release granules and its preparation, can solve the problems of environmental pollution, increase cost investment, etc., achieve high spreading uniformity, reduce repeated use, reduce The effect of cost input
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] A clothianidin sustained-release granule, comprising the following formula components in parts by mass:
[0036] 40 parts of anhydrous calcium sulfate powder, 30 parts of kaolin, 5 parts of other loading materials, 2 parts of clothianidin, 1.5 parts of white carbon black, 1 part of color adjustment agent, 5 parts of curing agent, 5 parts of internal replacement agent, one-way 0.01 part of permeable membrane, 0.01 part of glutaraldehyde, 1 part of magnesium amino acid chelate and 2 parts of water.
[0037] The preparation method of described a kind of clothianidin sustained-release granule is as follows:
[0038] (1) According to the composition of the formula, weigh the internal replacement agent and prepare small portions of equal proportions, weigh water, curing agent and glutaraldehyde respectively and stir until uniform, then add the small portion of the internal replacement agent and the one-way filter membrane, Stir for 15 minutes to obtain substance A, add magne...
Embodiment 2
[0047] A clothianidin sustained-release granule, comprising the following formula components in parts by mass:
[0048] 45 parts of anhydrous calcium sulfate powder, 35 parts of kaolin, 10 parts of other loading materials, 2.2 parts of clothianidin, 2 parts of white carbon black, 1.5 parts of color adjustment agent, 32 parts of curing agent, 10 parts of internal replacement agent, one-way 2.46 parts of filter membrane, 2.46 parts of formaldehyde, 3 parts of magnesium amino acid chelate and 3.3 parts of natural water.
[0049] The preparation method of described a kind of clothianidin sustained-release granule is as follows:
[0050](1) According to the ingredients of the formula, weigh the internal replacement agent and prepare small portions of equal proportions, respectively weigh the natural water, curing agent and formaldehyde and stir until uniform, then add the small portion of the internal replacement agent and the one-way filter membrane, Stir for 20 minutes to obtain...
Embodiment 3
[0060] A clothianidin sustained-release granule, comprising the following formula components in parts by mass:
[0061] 50 parts of anhydrous calcium sulfate powder, 40 parts of kaolin, 15 parts of other loading materials, 2.4 parts of clothianidin, 2.5 parts of white carbon black, 2 parts of color adjustment agent, 60 parts of curing agent, 15 parts of internal replacement agent, one-way 5 parts of filter membrane, 5 parts of titanium dioxide, 5 parts of magnesium amino acid chelate and 5 parts of water.
[0062] The preparation method of described a kind of clothianidin sustained-release granule is as follows:
[0063] (1) According to the composition of the formula, weigh the internal replacement agent and prepare small portions of equal proportions. Weigh the water, curing agent and titanium dioxide and stir until uniform, then add the small portion of the internal replacement agent and the one-way filter membrane. Stirring time 25min, obtain substance A, add amino acid c...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com