Concrete pumping retarder
A concrete pump and retarder technology, applied in the field of concrete admixtures, can solve the problems of unstable control of setting time, prolonging the setting time of cement, and slowing down the hydration speed of cement, so as to improve frost resistance and corrosion resistance, reduce water High rate, reduce the effect of bleeding rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] (1) Add 15 parts of polyacrylamide and 12 parts of fatty alcohol polyoxyethylene ether to 45 parts of soybean molasses, heat to 65°C and keep stirring for 15 minutes, then add 10 parts of saponin powder and 10 parts of tea seed powder, and continue heating until Stir at 95°C for 20 minutes, and cool to room temperature to obtain material I;
[0024] (2) Add 15 parts of modified starch, 12 parts of microcrystalline cellulose, 15 parts of coconut oil and 350 parts of water to 18 parts of volcanic ash, mix well and let stand at 0-5°C for 30 minutes, then add 8 parts of nano glue Powder and 6 parts of polyurethane, ultrasonic treatment at ultrasonic frequency 40kHz, power 100W for 20min, to obtain material II;
[0025] (3) Add material I, 30 parts of isomalt, 20 parts of sulfonated melamine, 9 parts of naphthalene-based water reducer and 6 parts of palmitic acid to material II, mix well and microwave under microwave frequency 2450MHz and power 600W Treat for 15 minutes, th...
Embodiment 2
[0029] (1) Add 17 parts of polyacrylamide and 15 parts of fatty alcohol polyoxyethylene ether to 50 parts of soybean molasses, heat to 70°C and keep stirring for 15 minutes, then add 12 parts of saponin powder and 10 parts of tea seed powder, and continue heating until Stir at 90°C for 15 minutes, and cool to room temperature to obtain material I;
[0030] (2) Add 20 parts of modified starch, 15 parts of microcrystalline cellulose, 15 parts of coconut oil and 400 parts of water to 20 parts of volcanic ash, mix well and let stand at 0-5°C for 30 minutes, then add 10 parts of nano glue Powder and 8 parts of polyurethane, ultrasonic treatment at ultrasonic frequency 40kHz, power 100W for 20min, to obtain material II;
[0031] (3) Add material I, 40 parts of isomalt, 25 parts of sulfonated melamine, 10 parts of naphthalene-based water reducer and 8 parts of palmitic acid to material II, mix well and microwave under microwave frequency 2450MHz and power 600W Treat for 15 minutes, ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com