Plant oil-based defoamer and preparation method of same
A defoamer, oil-based technology, applied in the field of vegetable oil-based defoamer and its preparation, can solve the problems of non-renewability and degradation, system compatibility, dispersion system stability, low defoaming and anti-foaming performance , to achieve good anti-foam effect and good system compatibility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Combine 45g palm oil and 5g specific surface area to 80m 2 / g of precipitation hydrophobic silica was added to the reaction flask, stirred, slowly heated to 120°C, kept for 1h, and then cooled to 40°C to obtain silica ointment. In addition, add 20g EBS, 60g aluminum hexadecanoate and 800g palm oil into the beaker, turn on the stirring and slowly raise the temperature to 150°C, keep it for 3h, lower the temperature to 30°C, quickly stir at 800r / min for 1h, add the white prepared in the previous step After the carbon black ointment is uniformly stirred, add 20g CD-50 (Guangdong Petrochemical Research Institute), 30g isotridecyl polyoxyethylene (5) ether and 15g secondary alcohol polyoxyethylene ether (15-S-7) and mix Evenly, defoamer I is obtained.
Embodiment 2
[0030] Make 55g palm oil and 6g specific surface area 120m 2 / g of precipitation hydrophobic silica was added to the reaction flask, stirred, slowly heated to 120°C, kept for 1h, and then cooled to 40°C to obtain silica ointment. Add 70g bis(octadecanoic acid) aluminum and 820g castor oil into the beaker, turn on the stirring and slowly raise the temperature to 130°C, keep it for 2h, lower the temperature to 30°C, quickly stir at 800r / min for 0.5h, add the white prepared in the previous step After the carbon black ointment is evenly stirred, add 30g of butanol polyoxyethylene (10) ether, 15g of EO / PO front copolymer (L61) and 45g of polyoxyethylene sorbitan monooleate (Tween-80) and mix Evenly, defoamer II is obtained.
Embodiment 3
[0032] Add 20g EBS, 60g bis(octadecanoic acid) aluminum and 820g castor oil into the beaker, turn on the stirring and slowly raise the temperature to 150℃, keep it for 2h, lower the temperature to 30℃, quickly stir at 800r / min for 0.5h, add 30g BYK-024 (Germany BYK), 20g butanol polyoxyethylene (10) ether, 25g isomeric tridecanol polyoxyethylene (5) ether and 20g polyoxyethylene sorbitan monooleate (Tween-80) Mix evenly to obtain defoamer III.
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com