A contact material, zirconium carbide copper technology, applied in the direction of contacts, circuits, electric switches, etc., can solve the constraints on the development of silver-based low-voltage electrical contact materials, wear resistance, insufficient oxidation resistance, shortage of silver resources, etc. question
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] Embodiment 1: Zirconium carbide copper-based contact material for low-voltage electrical appliances, its composition is by weight percentage: 5% zirconium carbide, 0.5% aluminum, 0.5% chromium, 0.5% zirconium, 1% rhenium oxide, 1% lanthanum oxide, and the rest for copper. The contact material processing method is as follows: Fully mix the powders of zirconium carbide, aluminum, chromium, zirconium, rhenium oxide, lanthanum oxide and copper in the above weight percentages, and grind to obtain an ultrafine mixed powder below 200 mesh; Put the superfine mixed powder obtained above into an airtight container and press it into the columnar billet required for processing with a cold isostatic press. The working pressure of the cold isostatic press is 250MPa, and the pressure is maintained for 3 minutes; The billets are sintered under protective gas at a sintering temperature of 1100°C for 2 hours; The sintered blank is formed by extrusion or forging, and then rolled to ...
Embodiment 2
[0012] Embodiment 2: Zirconium carbide copper-based contact material for low-voltage electrical appliances, its composition is by weight percentage: 2% zirconium carbide, 1% nickel, 2% samarium oxide, and the balance is copper. The contact material processing method is as follows: Fully mix the powders of zirconium carbide, nickel, samarium oxide and copper in the above percentage by weight, and grind to obtain an ultrafine mixed powder below 200 mesh; Put the superfine mixed powder obtained above into an airtight container and press it into the columnar billet required for processing with a cold isostatic press. The working pressure of the cold isostatic press is 200 MPa, and the pressure is maintained for 3 minutes; The billet is sintered under protective gas, the sintering temperature is 1000°C, and the time is 2.5 hours; The sintered blank is formed by extrusion or forging, and then rolled to form the contact material.
[0013] The zirconium carbide copper-based cont...
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
hardness | aaaaa | aaaaa |
electrical resistivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com