Antistatic composite calcium carbonate and preparation method thereof
A composite calcium carbonate and antistatic technology, which is applied in chemical instruments and methods, other chemical processes, dyed low-molecular organic compound treatment, etc., can solve the problems of composite material mechanical properties decline, different interface properties, uniform and strong dispersion, etc., to achieve The effect of high application value, low production cost and stable quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] An antistatic composite calcium carbonate and a preparation method thereof, comprising the following raw materials in parts by weight: 50 parts of calcium carbonate, 2 parts of modified polyurethane resin, 1 part of chlorinated rubber resin, 1 part of wax powder, 3 parts of barium sulfate, and acrylic ester 4 parts, 2 parts of cyclohexane, 1 part of ethylene glycol ether, 1 part of butanol, 5 parts of modifier, and appropriate amount of water; wherein the modifier is made of the following parts by weight of raw materials: 30 parts of nano titanium dioxide, 2 parts of montmorillonite powder, 3 parts of glutaraldehyde, 2 parts of pure acrylic emulsion, 1 part of alkyl quaternary ammonium salt, 3 parts of disodium hydrogen phosphate, 2 parts of cyclohexanone;
[0018] The preparation method includes the following steps:
[0019] (1) Mix calcium carbonate, modified polyurethane resin, chlorinated rubber resin, and wax powder evenly into the sand mill, grind to 300-400 mesh, and ...
Embodiment 2
[0024] An antistatic composite calcium carbonate and a preparation method thereof, comprising the following parts by weight of raw materials: 80 parts of calcium carbonate, 4 parts of modified polyurethane resin, 3 parts of chlorinated rubber resin, 3 parts of wax powder, 5 parts of barium sulfate, and acrylate 6 parts, 3 parts of cyclohexane, 1.5 parts of ethylene glycol ether, 2 parts of butanol, 8 parts of modifier, and appropriate amount of water; wherein the modifier is made of the following parts by weight of raw materials: 50 parts of nano titanium dioxide, 4 parts of montmorillonite powder, 5 parts of glutaraldehyde, 5 parts of pure acrylic emulsion, 3 parts of alkyl quaternary ammonium salt, 5 parts of disodium hydrogen phosphate, 4 parts of cyclohexanone;
[0025] The preparation method includes the following steps:
[0026] (1) Mix calcium carbonate, modified polyurethane resin, chlorinated rubber resin, and wax powder evenly into the sand mill, grind to 300-400 mesh, an...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com