A technology for precipitating silica and pigment dispersants, applied in the field of pigment dispersants, can solve the problems of inability to achieve long-term dispersion and suspension of pigment particles, poor dispersant stability, pigment sedimentation, etc., to avoid pigment flocculation, ensure the effect of painting, The effect of enhancing fluidity and thermal stability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] (1) Add 5 parts of terpene resin and 3 parts of microcrystalline wax to 15 parts of amphiphilic precipitated silica, first heat to 90-100°C and mix for 5 minutes, then add 4 parts of hydrogenated castor oil and 1 part of nano rubber powder , continue to heat to 120-130 ° C and mix for 10 minutes to obtain material I;
[0019] (2) Add 6 parts of cetyl ethylhexanoate and 1 part of isooctyl oleate to 10 parts of isopropanol, heat it to reflux state for 10 minutes while stirring, then add 2 parts of turpentine and 1 part of titanic acid Ester coupling agent and 1 part of vulcanized lard, continue to reflux and keep stirring for 10 minutes to obtain material II;
[0020] (3) Add material I, 3 parts of polyethylene glycol 400 and 3 parts of sodium polyacrylate to material II, mix thoroughly and then microwave at microwave frequency 2450MHz and power 700W for 10min, and finally cool the mixture to 60-65 After ℃, add 5 parts of polyvinylpyrrolidone, 3 parts of sodium cocoyl gl...
Embodiment 2
[0023] (1) Add 5 parts of terpene resin and 4 parts of microcrystalline wax to 20 parts of amphiphilic precipitated silica, first heat to 90-100 ° C and mix for 5 minutes, then add 5 parts of hydrogenated castor oil and 0.5 parts of nano rubber powder , continue to heat to 120-130 ° C and mix for 10 minutes to obtain material I;
[0024] (2) Add 6 parts of cetyl ethylhexanoate and 2 parts of isooctyl oleate to 15 parts of isopropanol, heat it to reflux state for 10 minutes while stirring, then add 2 parts of turpentine and 1 part of titanic acid Ester coupling agent and 0.5 part of vulcanized lard, continue to reflux and keep stirring for 10 minutes to obtain material II;
[0025] (3) Add material I, 5 parts of polyethylene glycol 400 and 2 parts of sodium polyacrylate to material II, mix thoroughly and microwave at microwave frequency 2450MHz, power 700W for 10min, and finally wait for the temperature of the mixture to cool naturally to 60-65 After ℃, add 6 parts of polyviny...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com