Unlock instant, AI-driven research and patent intelligence for your innovation.

High-strength basalt fiber composite bar

A basalt fiber and high-strength technology, applied in glass manufacturing equipment, manufacturing tools, etc., can solve the problems of high energy consumption of glass fiber, non-recyclable glass fiber composite bars, and large environmental pollution, etc., to achieve corrosion resistance, air stability, The effect of good air stability and simple production steps

Inactive Publication Date: 2017-05-10
安徽梦谷纤维材料科技有限公司
View PDF5 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] In the existing field of composite materials, the fibers used as composite reinforcement mainly include glass fiber, carbon fiber, boron fiber, alumina fiber, silicon carbide fiber, polyethylene fiber, etc., but due to price constraints, most fibers are only available Used in the military field, only glass fiber is widely used in the civilian field, but in the actual application process, glass fiber still has certain defects as a composite reinforcement, such as: (1) the production process of glass fiber consumes a lot of energy, It is not conducive to energy saving and environmental protection; (2) The preparation process of glass fiber is harmful to the human body, especially the glass fiber wool will have an irritating effect on human skin, and cannot be decomposed or absorbed after being inhaled into the human body, which may cause lung diseases or even cancer; (3) Environmental pollution is high, and glass fiber composite bars cannot be recycled or naturally degraded after being discarded, which is not conducive to environmental protection, etc.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] A high-strength basalt fiber composite bar, the high-strength basalt fiber composite bar is a fiber bar made of basalt fibers treated with a surface treatment agent, then impregnated and solidified by a matrix resin;

[0018] The basalt fiber is made of the following components in parts by weight: basalt rock 120, nano-titanium carbide 0.2, ginger stone 0.5;

[0019] The matrix resin is made of polypropylene resin 8, vinyl ester resin 42 and rosin 1 in parts by weight.

Embodiment 2

[0021] A high-strength basalt fiber composite bar, the high-strength basalt fiber composite bar is a fiber bar made of basalt fibers treated with a surface treatment agent, then impregnated and solidified by a matrix resin;

[0022] The basalt fiber is made of the following components in parts by weight: basalt rock material 130, nano-titanium carbide 0.3, and ginger stone 0.6;

[0023] The matrix resin is made of polypropylene resin 10, vinyl ester resin 45 and rosin 2 in parts by weight.

Embodiment 3

[0025] A high-strength basalt fiber composite reinforcement, the high-strength basalt fiber composite reinforcement is a fiber reinforcement formed by basalt fibers being treated with a surface treatment agent, then impregnated and solidified by a matrix resin;

[0026] The basalt fiber is made of the following components in parts by weight: basalt rock material 125, nano-titanium carbide 0.25, and ginger stone 0.55;

[0027] The matrix resin is made of polypropylene resin 9, vinyl ester resin 43 and rosin 1.5 in parts by weight.

[0028] In the above-mentioned embodiment:

[0029] Further: the preparation method of the basalt fiber is: after the basalt rock material, nano-titanium carbide, and ginger stone are melted at 1480°C, the continuous fiber is drawn through a platinum-rhodium alloy drawing bushing at high speed.

[0030] Further: the diameter of the basalt fiber is 6-13 μm.

[0031] Further: The surface treatment agent is prepared by mixing Wolan treatment agent and...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
diameteraaaaaaaaaa
Login to View More

Abstract

The invention discloses a high-strength basalt fiber composite bar which is a fiber bar prepared by treating basalt fibers with a surface treating agent, immersing and curing by a matrix resin, wherein the basalt fibers are made of the following components: basalt stone, nano-titanium carbide and ginger-like rock; the matrix resin is prepared from polypropylene resin, vinyl ester resin and rosin. The basalt fiber composite bar according to the invention has strong mechanical properties and can be widely used in industrial and civil construction industries, petroleum industries, aviation industries and the like. The preparation method of the basalt fiber composite bar provided by the invention not only is simple and rapid in step, but also can realize large-scale industrial production, and is low in production cost.

Description

technical field [0001] The invention relates to the field of composite materials, in particular to a high-strength basalt fiber composite bar. Background technique [0002] In the existing field of composite materials, the fibers used as composite reinforcement mainly include glass fiber, carbon fiber, boron fiber, alumina fiber, silicon carbide fiber, polyethylene fiber, etc., but due to price constraints, most fibers are only available Used in the military field, only glass fiber is widely used in the civilian field, but in the actual application process, glass fiber still has certain defects as a composite reinforcement, such as: (1) the production process of glass fiber consumes a lot of energy, It is not conducive to energy saving and environmental protection; (2) The preparation process of glass fiber is harmful to the human body, especially the glass fiber wool will have an irritating effect on human skin, and cannot be decomposed or absorbed after being inhaled into ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C03B37/00C03C25/30C03C25/24
CPCC03B37/00C03C25/24C03C25/30
Inventor 钱立兵李宁谈亚蓓