Modified acrylic resin energy-saving and environment-friendly coating material for cabinet of washing machine
An acrylic resin, energy-saving and environmentally friendly technology, applied in the field of coatings, can solve the problems of poor dispersion, poor heat resistance, low adhesion, etc., and achieve the effect of strong anti-aging performance, good gloss and enhanced adhesion.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] A modified acrylic resin energy-saving and environment-friendly coating for washing machine cabinets proposed by the present invention comprises the following raw materials in parts by weight: 40 parts of thermosetting acrylic resin, 28 parts of water-based epoxy resin, 25 parts of water-based polyurethane resin, and 1.8 parts of graphene oxide , 4 parts of magnesium oxide, 2 parts of nano-silica, 6 parts of expanded graphite, 5 parts of kaolin, 1.5 parts of polysorbate, 3 parts of water-based defoamer, 2 parts of water-based rust inhibitor, 2 parts of benzoic acid, 12 parts of polyol parts, 30 parts of water.
[0019] Its preparation method comprises the following steps:
[0020] S1. Heat the thermosetting acrylic resin with the specific gravity to 120°C, add the graphene oxide with the specific gravity, oscillate ultrasonically for 1.8 hours, and mix uniformly to obtain the modified acrylic resin;
[0021] S2. Mix the modified acrylic resin, water-based epoxy resin a...
Embodiment 2
[0025] A modified acrylic resin energy-saving and environment-friendly coating for washing machine cabinets proposed by the present invention comprises the following raw materials in parts by weight: 38 parts of thermosetting acrylic resin, 32 parts of water-based epoxy resin, 18 parts of water-based polyurethane resin, and 1 part of graphene oxide , 3 parts of magnesium oxide, 1.5 parts of nano-silica, 4 parts of expanded graphite, 7 parts of kaolin, 3 parts of polyoxyethylene sorbitan monolaurate, 2.5 parts of water-based defoamer, 4 parts of water-based rust inhibitor, 5 parts of benzoic acid, 18 parts of polyol, 25 parts of water.
[0026] Its preparation method comprises the following steps:
[0027] S1. Heat the thermosetting acrylic resin with the specific gravity to 115°C, add the graphene oxide with the specific gravity, oscillate ultrasonically for 1.5 hours, and mix uniformly to obtain a modified acrylic resin;
[0028] S2. Mix the modified acrylic resin, water-bas...
Embodiment 3
[0032] A modified acrylic resin energy-saving and environment-friendly coating for washing machine cabinets proposed by the present invention comprises the following raw materials in parts by weight: 20 parts of thermosetting acrylic resin, 20 parts of water-based epoxy resin, 30 parts of water-based polyurethane resin, and 2 parts of graphene oxide , 2 parts of magnesium oxide, 3 parts of nano-silica, 8 parts of expanded graphite, 6 parts of kaolin, 1 part of fatty acid glyceride, 2 parts of water-based defoamer, 3 parts of water-based rust inhibitor, 1 part of benzoic acid, 10 parts of polyol parts, 50 parts of water.
[0033] Its preparation method comprises the following steps:
[0034] S1. Heat the thermosetting acrylic resin with the specific gravity to 135° C., add the graphene oxide with the specific gravity, oscillate ultrasonically for 1 hour, and mix uniformly to obtain a modified acrylic resin;
[0035] S2. Mix the modified acrylic resin, water-based epoxy resin a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com