Textile assistant added with ethyl vanillin and preparation method of textile assistant
A technology of ethyl vanillin and textile auxiliaries, used in textiles and papermaking, fiber processing, flame retardant fibers, etc., can solve the problems of poor use effect, lack of environmental protection performance, low technology content, etc., and achieve practicality. Strong, excellent flame retardant effect, cheap raw material effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] (1) Accurately weigh 40 parts of hydroxypropyl methylcellulose, 30 parts of ethyl vanillin, 28 parts of styrene-butadiene transparent impact resin, 20 parts of sodium methylene dinaphthalene sulfonate, Nordimethacrylate 13 parts, diphenyltridecyl phosphite 10 parts, sorbitan ester 8 parts, lupeyl palmitate 6 parts, cocamidopropyl betaine 4 parts, peroxycarbonic acid 2 parts of ester, 2 parts of potassium ricinoleate, 1 part of polyferric sulfate, 3 parts of palmitic acid, 3 parts of methylenebisacrylamide, 100 parts of deionized water;
[0023] (2) Add sodium methylene dinaphthalene sulfonate, peroxycarbonate, potassium ricinoleate, and polyferric sulfate into the ball mill, mill for 1 hour, then add deionized water to the ball-milled mixture, and stir at 1000 rpm Stir for 2 hours at a high speed to obtain a preliminary mixed solution;
[0024] (3) Send the preliminary mixed solution into the reaction kettle, add styrene-butadiene transparent impact resin, quinol dimet...
Embodiment 2
[0028] (1) Accurately weigh 45 parts of hydroxypropyl methylcellulose, 33 parts of ethyl vanillin, 30 parts of styrene-butadiene transparent impact resin, 22 parts of sodium methylene dinaphthalene sulfonate, 16 parts of nordimethacrylate, 12 parts of diphenyltridecyl phosphite, 10 parts of sorbitan ester, 8 parts of lupeyl palmitate, 5 parts of cocamidopropyl betaine, peroxycarbonic acid 3 parts of potassium ricinoleate, 3 parts of potassium ricinoleate, 2 parts of polyferric sulfate, 4 parts of citric acid, 4 parts of polyethylene glycol dimethacrylate, 100 parts of deionized water;
[0029] (2) Add sodium methylene dinaphthalene sulfonate, peroxycarbonate, potassium ricinoleate, and polyferric sulfate into the ball mill, mill for 1.5 hours, then add deionized water to the ball-milled mixture, and stir at 1500 rpm Stir for 2.5 hours at a high speed to obtain a preliminary mixed solution;
[0030] (3) Send the preliminary mixed solution into the reaction kettle, add styrene-...
Embodiment 3
[0034] (1) Accurately weigh 50 parts of hydroxypropyl methylcellulose, 36 parts of ethyl vanillin, 32 parts of transparent impact-resistant resin of butylbenzene, 25 parts of sodium methylene dinaphthalene sulfonate, Nordimethacrylate 19 parts, diphenyltridecyl phosphite 14 parts, sorbitan ester 12 parts, lupeyl palmitate 10 parts, cocamidopropyl betaine 6 parts, carbonic acid peroxide 4 parts of ester, 4 parts of potassium ricinoleate, 3 parts of polyferric sulfate, 5 parts of linoleic acid, 5 parts of ethylene glycol diglycidyl ether, 100 parts of deionized water;
[0035] (2) Add sodium methylene dinaphthalene sulfonate, peroxycarbonate, potassium ricinoleate, and polyferric sulfate into a ball mill, mill for 2 hours, then add deionized water to the ball-milled mixture, and stir at 2000 rpm Stir for 3 hours at a high speed to obtain a preliminary mixed solution;
[0036] (3) Send the preliminary mixed solution into the reaction kettle, add styrene-butadiene transparent imp...