Unlock instant, AI-driven research and patent intelligence for your innovation.

Treatment method for tungsten mineral material roasting flue gas spraying waste water

A technology of mineral raw materials and treatment methods, which is applied in gaseous discharge wastewater treatment, multi-stage water treatment, water/sewage treatment, etc., can solve the problem of stable discharge of wastewater that is not easy to mix production, increase the cost of comprehensive wastewater treatment, and increase mixed wastewater. Dealing with problems such as difficulty, to achieve continuous and stable discharge standards, reduce treatment difficulty, and reduce treatment costs

Pending Publication Date: 2017-08-11
JIANGXI RARE EARTH & RARE METALS TUNGSTEN GRP HLDG CO LTD
View PDF6 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] The amount of waste water sprayed by flue gas spraying of tungsten mineral raw materials is small, but its composition is very complex and difficult to treat
The existing technology is usually combined with other production wastewater for joint treatment, which greatly increases the difficulty of mixed wastewater treatment, increases the cost of comprehensive wastewater treatment, and is not easy to achieve stable discharge of mixed production wastewater.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Treatment method for tungsten mineral material roasting flue gas spraying waste water

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] 1. After the primary solid-liquid separation, the COD concentration in the filtrate is 10123mg / L, and the arsenic concentration is 830mg / L.

[0028] 2. Add calcium hydroxide solution to the filtrate at room temperature to make slag, and perform secondary solid-liquid separation after reacting for 1 hour.

[0029] 3. After secondary solid-liquid separation, adjust the pH value of the solution system to 10 with sulfuric acid, and add 30% hydrogen peroxide to oxidize for 48 hours at the same time, and the volume ratio of the hydrogen peroxide to the filtrate is 1:10.

[0030] 4. Take 100 mL of the solution obtained in step 3, add 15 mL of ferric chloride solution and 10 mL of calcium chloride solution, react for 0.5 hours, and perform three-stage solid-liquid separation. The concentrations of the ferric chloride and calcium chloride solutions are both 10%.

[0031] 5. After the three-stage solid-liquid separation, the COD concentration in the filtrate is 325mg / L, the arse...

Embodiment 2

[0033] 1. After the primary solid-liquid separation, the COD concentration in the filtrate is 10123mg / L, and the arsenic concentration is 830mg / L.

[0034] 2. Add calcium hydroxide solution to the filtrate at room temperature to make slag, and perform secondary solid-liquid separation after reacting for 1 hour.

[0035] 3. After secondary solid-liquid separation, adjust the pH value of the solution system to 10 with sulfuric acid, and add 30% hydrogen peroxide to oxidize for 48 hours at the same time, and the volume ratio of the hydrogen peroxide to the filtrate is 1:10.

[0036] 4. Take 100 mL of the solution obtained in step 3, add 25 mL of ferric chloride solution and 10 mL of calcium chloride solution, react for 0.5 hours, and perform three-stage solid-liquid separation. The concentrations of the ferric chloride and calcium chloride solutions are both 10%.

[0037] 5. After the three-stage solid-liquid separation, the COD concentration in the filtrate is 300mg / L, the arse...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides a treatment method for tungsten mineral material roasting flue gas spraying waste water. The tungsten mineral material roasting flue gas spraying waste water mainly contains COD, heavy metal elements and other pollution factors difficult to remove. The invention provides a method capable of reducing COD, heavy metal elements and other pollution factors in the tungsten mineral material roasting flue gas spraying waste water, treated waste water can be up to the standard and discharged or converge with other production waste water, and discharged waste water can be up to the standard stably. The treatment method for the tungsten mineral material roasting flue gas spraying waste water specifically comprises procedures including primary solid-liquid separation, slagging, secondary solid-liquid separation, acid adjustment for oxidation, removal of heavy metals and tertiary solid-liquid separation, and the COD removal rate and the arsenic removal rate reach 96% and 99% or higher respectively after the waste water is treated.

Description

technical field [0001] The invention relates to a method for treating tungsten mineral raw material roasting flue gas spray wastewater, in particular to a treatment method for complex component tungsten mineral raw material roasting flue gas spray wastewater in the process of producing APT by extraction method, and belongs to the field of environmental protection chemical industry. Background technique [0002] Tungsten mineral raw materials are mainly used in the production of ammonium paratungstate. The current production methods of ammonium paratungstate mainly include ion exchange method and extraction method, and among the two processing methods, ion exchange method is the main method. The ammonium paratungstate produced by the extraction method has the characteristics of high product quality and environmental friendliness. With the development, production and application expansion of back-end high-quality tungsten products, under the background of the current resource-s...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C02F9/04C02F103/18
CPCC02F9/00C02F2301/08C02F1/001C02F1/72C02F1/722C02F1/76C02F1/66C02F1/52C02F2103/18
Inventor 徐双谢金明廖为鸿其他发明人请求不公开姓名
Owner JIANGXI RARE EARTH & RARE METALS TUNGSTEN GRP HLDG CO LTD