An environment-friendly, coating technology, applied in coatings, protein coatings, etc., can solve problems such as human skin, eye damage, human hazards, environmental impacts, etc., to achieve not easy to fade or change color, long service life, excellent hardness and the effect of abrasion resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] The preparation method of coating for environment-friendly building materials comprises the following steps:
[0021] (1) 20 parts of rutile nanoscale titanium dioxide, 25 parts of molecular sieves, 2 parts of graphene, and 10 parts of calcium oxide are evenly mixed in proportion to form a silty mixture;
[0022] (2) 15 parts of ferric chloride and 8 parts of potassium / zinc salt are dissolved in water to form an aqueous solution, and ethanol is added to the aqueous solution until solid precipitates begin to appear, and the temperature is raised until the solid precipitates are completely dissolved;
[0023] (3) Add the silty mixture obtained in step (1) to the solution obtained in step (2);
[0024] (4) Under the condition that the temperature of the heat preservation system is 50-55°C, after stirring to form a uniformly dispersed suspension, quickly add 10 parts of edible gelatin while keeping stirring to form a colloidal coating, cool to room temperature, pack and sea...
Embodiment 2
[0027] The preparation method of coating for environment-friendly building materials comprises the following steps:
[0028] (1) 20 parts of rutile nanoscale titanium dioxide, 25 parts of molecular sieves, 3 parts of graphene, and 10 parts of calcium oxide are uniformly mixed in proportion to form a silty mixture;
[0029] (2) 20 parts of ferric chloride and 10 parts of potassium / zinc salt are dissolved in water to form an aqueous solution, and ethanol is added to the aqueous solution until solid precipitates begin to appear, and the temperature is raised until the solid precipitates are completely dissolved;
[0030] (3) Add the silty mixture obtained in step (1) to the solution obtained in step (2);
[0031] (4) Under the condition that the temperature of the heat preservation system is 50-55°C, after stirring to form a uniformly dispersed suspension, quickly add 15 parts of edible gelatin while keeping stirring to form a colloidal coating, cool to room temperature, pack and...
Embodiment 3
[0034] The preparation method of coating for environment-friendly building materials comprises the following steps:
[0035] (1) 20 parts of rutile nanoscale titanium dioxide, 25 parts of molecular sieves, 5 parts of graphene, and 10 parts of calcium oxide are evenly mixed in proportion to form a silty mixture;
[0036] (2) 20 parts of ferric chloride and 15 parts of potassium / zinc salt are dissolved in water to form an aqueous solution, and ethanol is added to the aqueous solution until solid precipitates begin to appear, and the temperature is raised until the solid precipitates are completely dissolved;
[0037] (3) Add the silty mixture obtained in step (1) to the solution obtained in step (2);
[0038] (4) Under the condition that the temperature of the heat preservation system is 50-55°C, after stirring to form a uniformly dispersed suspension, quickly add 15 parts of edible gelatin while keeping stirring to form a colloidal coating, cool to room temperature, pack and se...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com