Composite emulsifier and preparation method thereof
A compound emulsifier and emulsifier technology, applied in fuel additives, petroleum industry, liquid carbon-containing fuels, etc., can solve the problems of poor performance of chemical additives, high energy consumption, incomplete combustion, etc., and achieve environmental protection and pollution-free preparation process , The preparation process is simple, and the effect of promoting combustion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The emulsifier components include 10 parts by weight of acryl polyether, 8 parts of ethylene glycol, 2 parts of alkanolamide, 3 parts of isopropanol, 5 parts of n-decyl alcohol, and 7 parts of sodium dodecylbenzenesulfonate 8 parts, 8 parts of sodium bicarbonate, 4 parts of polyethylene glycol and 2 parts of cosolvent.
[0015] The preparation method of the present embodiment comprises the following steps:
[0016] A. After mixing acryl polyether, ethylene glycol, alkyl alcohol amide, and isopropanol, add it to a stirring tank and stir at a stirring rate of 400 rpm and a stirring time of 20 minutes to obtain a mixture A;
[0017] B. Add n-decyl alcohol, sodium dodecylbenzenesulfonate, sodium bicarbonate, polyethylene glycol and co-solvents to the mixture A, mix them and add them to the reaction kettle to heat the reaction. During the heating process, keep stirring, and the heating temperature The temperature is 40°C, the heating time is 10 minutes, and then the tempera...
Embodiment 2
[0020] The emulsifier components include 30 parts by weight of acryl polyether, 15 parts of ethylene glycol, 8 parts of alkanolamide, 10 parts of isopropanol, 15 parts of n-decyl alcohol, and 17 parts of sodium dodecylbenzenesulfonate 18 parts, 18 parts of sodium bicarbonate, 10 parts of polyethylene glycol and 8 parts of cosolvent.
[0021] The preparation method of the present embodiment comprises the following steps:
[0022] A. After mixing acryl polyether, ethylene glycol, alkyl alcohol amide, and isopropanol, add it to a stirring tank and stir at a stirring rate of 400 rpm and a stirring time of 20 minutes to obtain a mixture A;
[0023] B. Add n-decyl alcohol, sodium dodecylbenzenesulfonate, sodium bicarbonate, polyethylene glycol and co-solvents to the mixture A, mix them and add them to the reaction kettle to heat the reaction. During the heating process, keep stirring, and the heating temperature The temperature is 40°C, the heating time is 10 minutes, and then the ...
Embodiment 3
[0026] The emulsifier components include 15 parts of acryl polyether, 10 parts of ethylene glycol, 3 parts of alkanolamide, 4 parts of isopropanol, 6 parts of n-decyl alcohol, and 9 parts of sodium dodecylbenzenesulfonate in parts by weight. 10 parts, 10 parts of sodium bicarbonate, 5 parts of polyethylene glycol and 3 parts of cosolvent.
[0027] The preparation method of the present embodiment comprises the following steps:
[0028] A. After mixing acryl polyether, ethylene glycol, alkyl alcohol amide, and isopropanol, add it to a stirring tank and stir at a stirring rate of 400 rpm and a stirring time of 20 minutes to obtain a mixture A;
[0029] B. Add n-decyl alcohol, sodium dodecylbenzenesulfonate, sodium bicarbonate, polyethylene glycol and co-solvents to the mixture A, mix them and add them to the reaction kettle to heat the reaction. During the heating process, keep stirring, and the heating temperature The temperature is 40°C, the heating time is 10 minutes, and the...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com