A method of preparing expanded graphite or graphene with electrolytic aluminum waste cathode carbon
A technology of expanded graphite and waste cathode, which is applied in the direction of graphene, chemical instruments and methods, nano-carbon, etc., can solve the problems of high energy consumption, no report in research or practice, environmental pollution of electrolytic aluminum waste cathode carbon blocks, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0066] The electrolytic aluminum waste cathode charcoal used in the embodiment of the present invention is taken from the electrolytic cell waste cathode charcoal dismantled in the overhaul of an aluminum plant, and its main chemical components are: C 58.73%, F 9.88%, Na 11.87%, Al 2.44%, Fe 0.75%, Si 4.33%, Ca1.39%, Mg 0.56%, cyanide content 0.22%; The strong oxidizing agent used in the embodiment of the present invention is ZC-HO3 type strong oxidizing agent (by potassium ferrate, potassium dichromate and secondary Potassium chlorate is made in a mass ratio of 2:1:4), purchased from Hunan Xiaoyin Wuji Environmental Energy Technology Development Co., Ltd.; the purity of the hydrazine used in the examples of the present invention is 98.5%.
[0067] (1) Hydrothermal oxidation to produce graphite oxide slurry: crush 10kg of electrolytic aluminum waste cathode carbon to a particle size of less than 6mm, then place it together with 4kg of ZC-HO3 strong oxidant in an oxidation tank ...
Embodiment 2
[0078] The waste cathode charcoal used in the embodiment of the present invention is taken from the bulk electrolytic aluminum waste cathode charcoal stored in the warehouse of an aluminum factory, and its main chemical components are: C 68.03%, F 8.05%, Na 9.21%, Al 2.07% , Fe 0.55%, Si 3.11%, Ca1.14%, Mg 0.57%, cyanide content 0.18%; The strong oxidant used in the embodiment of the present invention is ZC-HO3 type oxidant (by potassium ferrate, potassium dichromate and Potassium hypochlorite is made with a mass ratio of 2:1:4), purchased from Hunan Xiaoyin Wuji Environmental Energy Technology Development Co., Ltd.; the purity of the hydrazine used in the examples of the present invention is 98.5%.
[0079] (1) Hydrothermal oxidation to produce graphite oxide slurry: crush 10kg of electrolytic aluminum waste cathode carbon to a particle size of less than 5mm, then place it in an oxidation tank with a wet grinding mechanism together with 4.8kg of ZC-HO3 strong oxidant, add 90kg...
Embodiment 3
[0090] The electrolytic aluminum waste cathode charcoal used in the embodiment of the present invention is taken from the electrolytic cell waste cathode charcoal dismantled in the overhaul of an aluminum plant, and its main chemical components are: C 58.56%, F 9.86%, Na 11.86%, Al 2.42%, Fe 0.74%, Si 4.33%, Ca1.36%, Mg 0.57%, cyanide content 0.22%; The strong oxidant used in the embodiment of the present invention is ZC-HO3 type oxidant (by potassium ferrate, potassium dichromate and potassium hypochlorite Made at a mass ratio of 2:1:4), purchased from Hunan Xiaoyin Wuji Environmental Energy Technology Development Co., Ltd.; the purity of the hydrazine used in the examples of the present invention is 98.5%.
[0091] (1) Supercritical / liquid carbon dioxide oxidative fluorination conversion: crush 10kg of electrolytic aluminum waste cathode carbon to a particle size below 5mm, then place it in a leaching tank with a rolling and mixing mechanism, use 100kg of liquid carbon dioxid...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle diameter | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| density | aaaaa | aaaaa |