[0056] Each of the following material components is measured in parts by mass.
[0057] (1) After mixing 100 parts of water and 2 parts of sodium dodecylsulfonate, adjust the pH to 8-9 with ammonia water; then add 3 parts of styrene monomer, 1 part of butyl acrylate, 10 parts of methacrylic acid and 10 parts of acrylamide After emulsifying at a speed of 100rpm for 15 minutes, it was in a homogeneous state; the temperature was raised to 75°C, and 2 parts of ammonium persulfate (made into a 10% (w / w) aqueous solution, i.e. 20 parts) was added dropwise, reacted for 3 hours, and then added Stabilizer (polyvinyl alcohol 1799) 2 parts, mixed to obtain a dispersant. Adjust the dispersant concentration to 40% with water.
[0058] (2) Dispersion of toner: First, 200 parts of water, 8 parts of dispersant with a concentration of 40%, 60 parts of toner (Clariant blue toner, C.I.15:3 blue), grind and disperse until the particle size D50 of the color paste is in the range of 200 -500 nano...
Embodiment 2
[0064] Each of the following material components is measured in parts by mass.
[0065] (1) After mixing 50 parts of water and 2 parts of sodium dodecyl sulfonate, adjust the pH to 8-9 with sodium hydroxide solution; then add 3 parts of styrene monomer, 1 part of butyl acrylate, 10 parts of acrylic acid, and acrylamide 5 parts and 5 parts of maleic anhydride, after emulsification at 200rpm for 15 minutes, it was in a homogeneous state; the temperature was raised to 70°C, and 2 parts of ammonium persulfate was added dropwise (to make a 10% (w / w) aqueous solution, i.e. 20 parts) , reacted for 2.5 hours, then added 2 parts of stabilizer (commercially available sodium carboxymethylcellulose, Guangzhou Daojun Biotechnology Co., Ltd.), and mixed to obtain a dispersant. Adjust the dispersant concentration to 40% with water.
[0066] (2) Dispersion of toner: First, 200 parts of water, 12 parts of dispersant with a concentration of 40%, and 70 parts of toner (BASF blue toner (C.I.60 b...
Embodiment 3
[0072] Each of the following material components is measured in parts by mass.
[0073] (1) After mixing 150 parts of water and 2 parts of sodium dodecylsulfonate, adjust the pH to 8-9 with ammonia water; then add 3 parts of styrene monomer, 1 part of butyl acrylate, 10 parts of methacrylic acid, and 5 parts of acrylamide and 5 parts of hydroxypropyl acrylate, after emulsification at 150rpm for 15 minutes, it was in a homogeneous state; the temperature was raised to 80°C, and 2 parts of ammonium persulfate was added dropwise (to make a 10% (w / w) aqueous solution, i.e. 20 parts) , reacted for 2 hours, then added 2 parts of stabilizer (polyvinyl alcohol 1799), and mixed to obtain a dispersant. Adjust the dispersant concentration to 40% with water.
[0074] (2) Dispersion of toner: First, 200 parts of water, 10 parts of dispersant with a concentration of 40%, and 63 parts of toner (BASF blue toner (C.I.60 blue)) are ground and dispersed until the particle size D50 of the color p...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com