A technology for absorbing odors and hydrocolloids, applied in the direction of adhesives, adhesive types, cellulose adhesives, etc., can solve the problem of less hydrocolloid materials that inhibit or absorb odors, achieve excellent self-adhesive performance, eliminate odors, The effect of overcoming psychological barriers
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Put 170 grams of rubber elastic body, 90 grams of plasticizer and zinc oxide into the sigma mixer according to the composition ratio in Table 2, and mix for 45 minutes at 150°C. Then at 140 DEG C, 250 grams of tackifier were added and continued to mix for 30 minutes. At a temperature of 120 DEG C, 490 grams of hydrophilic polymer sodium carboxymethyl cellulose CMC was dropped into the mixer, and continued to mix for 20 minutes.
[0027] The elastomer is Kraton's product polyethylene isoprene ethylene D1611.
[0028] The plasticizer is mineral oil or DOP.
[0029] The tackifier is C5 hydrocarbon petroleum resin of Clay Power.
[0030] The hydrophilic polymer is sodium carboxymethyl cellulose CMC of Ashland Company of the United States.
[0031] Zinc oxide was purchased from Aladdin Corporation.
Embodiment 2
[0032] Example 2 sample preparation
[0033] The hydrocolloid prepared by embodiment 1 is put into an extruder and extruded into a sheet with a thickness of 0.45mm, and simultaneously rolled and clad on the hydrocolloid sheet with polyurethane film and release paper to obtain a hydrocolloid dressing material.
Embodiment 3
[0034] Embodiment 3 water absorption test
[0035] Water absorption test: Cut the sample into a circular sample with a diameter of 1 inch with a cutter; stick the sample and PP synthetic paper with double-sided tape; remove the backing, weigh it, and place it in 60ml of test solution , Take it out at 2, 4, 6, 18, 24, 48, and 72 hours, and weigh it when it stops dripping, and measure it by water absorption.
[0036]
[0037] where W 2 Weigh the weight for the nth hour, W 1 It is the weight of the application sample and PP synthetic paper. The water absorption results are shown in Table 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com