Environmentally friendly paint containing shell powder and preparation method of paint
A shell powder, environment-friendly technology, applied in the field of coatings, achieves the effects of environmental protection, no chemical pollution, mosquito infestation, good moisture-proof effect, and comprehensive performance improvement.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0026] The present invention also provides a preparation method of an environment-friendly coating containing shell powder, comprising the following steps:
[0027] Step 1: Pulverize the shell powder, kaolin and porous starch respectively, and pass through a sieve of more than 300 mesh;
[0028] Step 2: adding 80-100 parts by weight of shell powder and 20-30 parts by weight of kaolin treated in step 1 into 80-100 parts by weight of water at a temperature of 90-100°C and adding 20-30 parts by weight of an emulsifier , stirred for 10 to 15 minutes, then added 40 to 70 parts by weight of biosynthetic binder for dispersion, added 5 to 8 parts by weight of dispersant and 1 to 3 parts by weight of citric acid monohydrate, and then heated to 90-95°C and heat preservation for 30-40 minutes, and the process of heat preservation is accompanied by stirring to obtain a slurry, wherein the biosynthetic binder contains the following components: konjac glucomannan, sodium alginate, starch ac...
Embodiment 1
[0034] A preparation method of an environment-friendly paint containing shell powder, comprising the following steps:
[0035] Step 1: Pulverize the shell powder, kaolin and porous starch respectively, and pass through a sieve of more than 300 mesh;
[0036] Step 2: Add 80g of shell powder and 20g of kaolin treated in step 1 into 80g of water at a temperature of 90°C, add 20g of emulsifier at the same time, stir for 10min, and then add 40g of biosynthetic binder to disperse. During the process, 5g of sodium hexametaphosphate and 1g of citric acid monohydrate were added, then heated to 90°C and kept warm for 30 minutes, and the process of keeping warm was accompanied by stirring to obtain a slurry, in which 40g of biosynthetic binder contained 15g of konjac Glucomannan, 5g sodium alginate, 2g starch acetate, 5g carboxymethyl chitosan, 3g polyvinyl alcohol and 10g water;
[0037] Step 3: Add 5g of mosquito repelling essential oils (1g each of lavender essential oil, Qilixiang e...
Embodiment 2
[0040] A preparation method of an environment-friendly paint containing shell powder, comprising the following steps:
[0041] Step 1: Pulverize the shell powder, kaolin and porous starch respectively, and pass through a sieve of more than 300 mesh;
[0042] Step 2: Add 100g of shell powder and 30g of kaolin treated in step 1 into 100g of water at a temperature of 100°C, add 30g of emulsifier at the same time, stir for 15min, and then add 70g of biosynthetic binder to disperse. During the process, 8g of sodium hexametaphosphate and 3g of citric acid monohydrate were added, then heated to 95°C and kept for 40 minutes, and the process of keeping warm was accompanied by stirring to obtain a slurry, in which 70g of biosynthetic binder contained 27g of konjac glucomannan Polysaccharide, 8.75g sodium alginate, 3.5g starch acetate, 8.75g carboxymethyl chitosan, 4.5g polyvinyl alcohol and 17.5g water;
[0043] Step 3: Add 10g of mosquito repellent essential oil (2g each of lavender e...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com