A technology of anti-corrosion synergist and preservative, which is applied in the field of anti-corrosion synergist containing branched non-ionic surfactant and quaternary ammonium salt surfactant, which can solve the problems of safety and drug resistance, etc. To achieve the effects of reducing toxicity, environmental protection and safety cost control, and good anti-corrosion effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] Put 14wt% of sucrose stearate, 2.8wt% of dodecyl pyridinium chloride, 1wt% of tea polyphenols, 1wt% of potassium chloride, 30wt% of methyl propylene glycol, and the remainder of deionized water into 3m 3 In the airflow mixer, the operating pressure of the compressed air is 0.8Mpa, and it is prepared after 3-5 minutes of mixing.
Embodiment 2
[0020] Put 20wt% of sucrose stearate, 4.5wt% of tetradecyltrimethylammonium bromide, 1.8wt% of tea polyphenols, 2wt% of potassium chloride, 40wt% of methyl propylene glycol, and the balance of deionized water into 3m 3 In the airflow mixer, the operating pressure of the compressed air is 0.8Mpa, and it is prepared after 3-5 minutes of mixing.
Embodiment 3
[0022] Put 25wt% of sucrose stearate, 5.8wt% of cetylpyridinium chloride, 3wt% of tea polyphenols, 3wt% of potassium chloride, 40wt% of methyl propylene glycol, and the remainder of deionized water into 3m 3 In the airflow mixer, the operating pressure of the compressed air is 0.8Mpa, and it is prepared after 3-5 minutes of mixing.