A kind of anti-slip glaze, anti-slip brick and preparation method thereof

A technology of anti-slip and surface glaze, which is applied in the field of ceramics, can solve the problems of potential safety hazards, structural strength not as good as ceramic floor tiles, and large environmental damage

Active Publication Date: 2021-05-11
HEYUAN DONGYUAN EAGLE CERAMICS CO LTD
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, natural stone has great damage to the environment, high cost, and its structural strength is often inferior to ceramic floor tiles, so more and more buildings choose to use ceramic floor tiles
However, ceramic floor tiles have a good effect of beautifying the environment because of their strong decorative properties, but because of their smooth surface, they are slippery when encountering water and cause safety hazards. pain, loss of property and impact on reputation

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • A kind of anti-slip glaze, anti-slip brick and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0038]First, prepare the base glaze. Bottom glaze comprises bottom glaze additive, also comprises bottom glaze raw material, bottom glaze frit and necessary water; In the present embodiment, bottom glaze raw material comprises: marble 8%, quartz 8%, boron oxide 11% in mass percentage , 12% zirconium silicate, 8% medium aluminum powder, 24% albite feldspar, 10% kaolin, 4% desilicate aluminum powder, 5% calcite, 10% dolomite; the base glaze frit is calculated by mass percentage, including: SiO2 65%, Al2O3 10.5%, CaO 10.25%, MgO 5.25%, K2O 2%, Na2O 7%; in other embodiments, the base glaze raw material and the base glaze frit can also be selected from other common ingredients. The bottom glaze additive is a C9 resin solution, and the C9 resin solution is a solution in which the solute is C9 resin, the solvent is ethylcyclohexane, and the mass concentration is 1%. The bottom glaze raw material accounts for 70% of the bottom glaze total mass, and the bottom glaze frit accounts for ...

Embodiment 2

[0043] First, prepare the base glaze. Bottom glaze comprises bottom glaze additive, also includes bottom glaze raw material, bottom glaze frit and necessary water; The composition of bottom glaze raw material and bottom glaze frit is identical with embodiment 1; Bottom glaze additive is C9 resin solution, and C9 resin solution is The solute is C9 resin, the solvent is ethylcyclohexane, and the solution with a mass concentration of 3%; the raw material of the bottom glaze accounts for 60% of the total mass of the bottom glaze, the frit of the bottom glaze accounts for 32% of the total mass of the bottom glaze, and the C9 resin solution accounts for 60% of the total mass of the bottom glaze. 2% of the total mass of the bottom glaze, the rest is water. After mixing, put it into the glaze machine and stir evenly to get the bottom glaze.

[0044] Second, prepare the top glaze. The surface glaze comprises a surface glaze additive, and also includes a surface glaze raw material, a ...

Embodiment 3

[0048] First, prepare the base glaze. Bottom glaze comprises bottom glaze additive, also includes bottom glaze raw material, bottom glaze frit and necessary water; The composition of bottom glaze raw material and bottom glaze frit is identical with embodiment 1; Bottom glaze additive is C9 resin solution, and C9 resin solution is The solute is C9 resin, the solvent is ethylcyclohexane, and the mass concentration is a solution of 2%; the base glaze raw material accounts for 60% of the total mass of the base glaze, the base glaze frit accounts for 32% of the total mass of the base glaze, and the C9 resin solution accounts for 60% of the total mass of the base glaze. 3% of the total mass of the bottom glaze, the rest is water. After mixing, put it into the glaze machine and stir evenly to get the bottom glaze.

[0049] Second, prepare the top glaze. The surface glaze comprises a surface glaze additive, and also includes a surface glaze raw material, a surface glaze frit and nec...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle size (mesh)aaaaaaaaaa
particle size (mesh)aaaaaaaaaa
thicknessaaaaaaaaaa
Login to View More

Abstract

The application provides an anti-slip glaze, an anti-slip brick and a preparation method. An anti-slip glaze comprises an anti-slip glaze additive compound A, the structural formula is: R is CH3 or F. An anti-skid brick comprises a body, a bottom glaze layer, a top glaze layer and an anti-skid glaze layer, the bottom glaze layer is arranged between the body and the top glaze layer, and the top glaze layer is arranged between the bottom glaze layer and the non-slip glaze layer. A method for preparing an anti-skid brick, comprising: forming a body, and then pouring an underglaze on the surface of the body to obtain a bottom glaze layer; pouring a top glaze on the surface of the bottom glaze layer to obtain a top glaze layer, and then performing inkjet printing; spraying anti-skid Glaze to obtain a non-slip glaze layer, and perform the fourth drying treatment to obtain pre-fired bricks; put the pre-fired bricks into the kiln and heat up to 1100‑1200 ° C for firing; then cool to room temperature to obtain semi-finished products, which are post-processed to get the finished product. The anti-slip brick prepared by using the anti-slip glaze and the preparation method provided by the application has good anti-slip performance, outstanding thermal shock resistance and antifouling performance.

Description

technical field [0001] The invention relates to the field of ceramics, in particular to an anti-slip glaze, an anti-slip brick and a preparation method thereof. Background technique [0002] The ground decoration of public buildings (hotels, office buildings, high-end apartments, etc.) is generally done by floor tiles. In terms of materials, people usually choose natural stone or ceramic floor tiles. However, natural stone has great damage to the environment, high cost, and is often inferior to ceramic floor tiles in terms of structural strength, so more and more buildings choose to use ceramic floor tiles. However, ceramic floor tiles have a good effect of beautifying the environment because of their strong decorative properties, but because of their smooth surface, they are slippery when encountering water and cause safety hazards. pain, loss of property and impact on reputation. [0003] The key to whether these properties of anti-slip tiles can be achieved is the anti-...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C03C8/14C03C8/20C03C8/02B28B11/04B28B11/00C04B41/89E04F13/14
CPCB28B11/001B28B11/044C03C8/02C03C8/14C03C8/20C04B41/52C04B41/89E04F13/14C04B41/504C04B41/5022
Inventor 陈贤伟廖花妹吴志坚程贵生李丽芳
Owner HEYUAN DONGYUAN EAGLE CERAMICS CO LTD