A paper-plastic composite bag and film preparation technology, applied in the field of packaging materials, can solve the problems of elongation at break not meeting demand, damage to health and living environment, and product quality not meeting requirements, etc. Promote development, good sealing effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for preparing a highly airtight film for a paper-plastic composite bag, comprising the steps of:
[0026] S1. Mix 20kg polytetrafluoroethylene and 20kg polyethylene terephthalate evenly, irradiate, and the irradiation dose is 400KGy, exhaust and degas, add 5kg talcum powder, 1kg silane coupling agent, and grind to The particle size is 20-40 μm, then add 100kg epoxy tall oil and stir for 10min, the stirring speed is 4500r / min, to obtain the first material;
[0027] S2. Stir 10kg of poly-β-hydroxybutyric acid, 80kg of polylactic acid, 22kg of microcrystalline cellulose, and 34kg of the first material for 10 minutes at a stirring speed of 1400r / min and a stirring temperature of 100°C to obtain a second material;
[0028] S3. Raise the temperature of 100kg of the second material to 140°C, add 1kg of polydimethylsiloxane, 1kg of methylphenyldiethoxysilane, 2kg of zinc stearate, 1kg of oxidized polyethylene wax, and 2kg of triallyl Isocyanuric acid ester, 1kg heat s...
Embodiment 2
[0031] A method for preparing a highly airtight film for a paper-plastic composite bag, comprising the steps of:
[0032] S1. Mix 40kg polytetrafluoroethylene and 10kg polyethylene terephthalate evenly, irradiate, and the irradiation dose is 460KGy, exhaust and degas, add 1kg talcum powder, 2kg silane coupling agent, and grind to The particle size is 20-40 μm, then add 60kg epoxy tall oil and stir for 16min, the stirring speed is 4200r / min, to obtain the first material;
[0033] S2. Stir 20kg of poly-β-hydroxybutyric acid, 40kg of polylactic acid, 35kg of microcrystalline cellulose, and 22kg of the first material for 16 minutes at a stirring speed of 1200r / min and a stirring temperature of 120°C to obtain the second material;
[0034] S3. Heat 80kg of the second material to 148°C, add 0.5kg of polydimethylsiloxane, 2kg of methylphenyldiethoxysilane, 1kg of zinc stearate, 2kg of oxidized polyethylene wax, and 1kg of triallyl Base isocyanuric acid ester, 2kg heat stabilizer con...
Embodiment 3
[0037] A method for preparing a highly airtight film for a paper-plastic composite bag, comprising the steps of:
[0038] S1. Mix 25kg polytetrafluoroethylene and 18kg polyethylene terephthalate evenly, irradiate, and the irradiation dose is 420KGy, exhaust and degas, add 4kg talcum powder, 1.2kg silane coupling agent, grind When the particle size is 20-40 μm, add 90kg epoxy tall oil and stir for 12min, and the stirring speed is 4400r / min to obtain the first material;
[0039] S2. Stir 12kg of poly-β-hydroxybutyric acid, 70kg of polylactic acid, 28kg of microcrystalline cellulose, and 30kg of the first material for 12 minutes at a stirring speed of 1350r / min and a stirring temperature of 105°C to obtain the second material;
[0040] S3. Raise the temperature of 95kg of the second material to 142°C, add 0.8kg of polydimethylsiloxane, 1.3kg of methylphenyldiethoxysilane, 1.7kg of zinc stearate, 1.4kg of oxidized polyethylene wax, 1.7 kg triallyl isocyanurate, 1.4kg heat stabili...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com