Cooking agent used for pulping in papermaking
A technology of cooking and pulping, which is applied in the field of papermaking, can solve the problems of low yield, heavy pollution, and environmental pollution, and achieve the effect of long usable life and good cooking effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] S1 prepares materials, cuts up the reed raw materials and removes impurities;
[0019] S2 One-time cooking: One-time cooking according to the liquid ratio of 1:4, the cooking temperature is 80℃, the cooking time is 15min, and the water is washed. The cooking liquid used, according to mass percentage, is composed of the following components: sodium hydroxide 6%, sodium sulfite 0.5%, 1.6% of sodium sulfide, 0.5% of anthraquinone, 0.03% of sodium dodecyl sulfonate, the balance water;
[0020] S3 Secondary cooking: Perform secondary cooking at a liquid ratio of 1:5. The cooking temperature is 60°C, the cooking time is 15 minutes, and the cooking time is 15 minutes. Wash with water. The cooking liquid used is obtained by diluting the cooking agent with water. The amount of water is 120 times that of the cooking agent. The cooking agent is prepared as follows: the graphene aerogel powder is dispersed in water to obtain a dispersion with a mass fraction of 15%, and the mixed enzyme...
Embodiment 2
[0022] S1 prepares materials, cuts up the reed raw materials and removes impurities;
[0023] S2 One-time cooking: One-time cooking according to the liquid ratio of 1:4, the cooking temperature is 80℃, the cooking time is 15min, and the water is washed. The cooking liquid used, according to mass percentage, is composed of the following components: sodium hydroxide 6%, sodium sulfite 0.5%, 1.6% of sodium sulfide, 0.5% of anthraquinone, 0.03% of sodium dodecyl sulfonate, the balance water;
[0024] S3 Secondary cooking: Perform secondary cooking at a liquid ratio of 1:5. The cooking temperature is 60°C, the cooking time is 15 minutes, and the cooking time is 15 minutes. Wash with water. The cooking liquid used is obtained by diluting the cooking agent with water. The amount of water is 120 times that of the cooking agent. The cooking agent is prepared by the following method: the graphene aerogel powder is dispersed in water to obtain a dispersion with a mass fraction of 18%, the mix...
Embodiment 3
[0026] S1 prepares materials, cuts up the reed raw materials and removes impurities;
[0027] S2 One-time cooking: One-time cooking according to the liquid ratio of 1:4, the cooking temperature is 80℃, the cooking time is 15min, and the water is washed. The cooking liquid used, according to mass percentage, is composed of the following components: sodium hydroxide 6%, sodium sulfite 0.5%, 1.6% of sodium sulfide, 0.5% of anthraquinone, 0.03% of sodium dodecyl sulfonate, the balance water;
[0028] S3 Secondary cooking: Perform secondary cooking at a liquid ratio of 1:5. The cooking temperature is 60°C, the cooking time is 15 minutes, and the cooking time is 15 minutes. Wash with water. The cooking liquid used is obtained by diluting the cooking agent with water. The amount of water is 120 times that of the cooking agent. The cooking agent is prepared by the following method: the graphene aerogel powder is dispersed in water to obtain a dispersion with a mass fraction of 12%, the mix...
PUM
Property | Measurement | Unit |
---|---|---|
quality score | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com