Wet-mixed mortar adjusting plasticizer
A wet-mixed mortar and plasticizer technology, applied in the field of concrete admixtures, can solve the problems of insufficient density of the mortar system, unfavorable mortar quality control, poor control of hydration speed, etc., to achieve improved storage stability and strong adhesion , the effect of high density
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0055] A wet-mix mortar regulating plasticizer, the wet-mix mortar regulating plasticizer is composed of the following raw materials in weight percentage: retarding component 18.40%, air-entraining component 10.0%, water-retaining component 0.20%, viscosity-increasing component 0.20% of water, 0.20% of anti-corrosion components and 71.00% of water;
[0056] Among them, the air-entraining component is composed of 57.14% by weight of sodium alkylbenzene sulfonate, 28.57% of sodium lauryl sulfate and 14.29% of triterpene saponins; the retarding component is composed of 83.34% by weight of glucose sodium tripolyphosphate, 8.33% white sugar and 8.33% sodium tripolyphosphate; the water-retaining component is composed of 50.00% hydroxypropyl methylcellulose and 50.00% sodium carboxymethyl cellulose; the antiseptic component is a compound Phenolics; the viscosity-enhancing component is polyethylene glycol.
Embodiment 2
[0058] A wet-mix mortar regulating plasticizer, the wet-mix mortar regulating plasticizer is composed of the following raw materials in weight percentage: retarding component 16.40%, air-entraining component 10.0%, water-retaining component 0.20%, viscosity-increasing component 0.20% of water, 0.20% of anti-corrosion components and 73.00% of water;
[0059] Among them, the air-entraining component is composed of 57.14% by weight of sodium alkylbenzene sulfonate, 28.57% of sodium lauryl sulfate and 14.29% of triterpene saponins; the retarding component is composed of 83.34% by weight of glucose sodium tripolyphosphate, 8.33% white sugar and 8.33% sodium tripolyphosphate; the water-retaining component is composed of 50.00% hydroxypropyl methylcellulose and 50.00% sodium carboxymethyl cellulose; the antiseptic component is a compound Phenolics; the viscosity-enhancing component is polyethylene glycol.
Embodiment 3
[0061] A wet-mix mortar regulating plasticizer, the wet-mix mortar regulating plasticizer is composed of the following raw materials in weight percentage: retarding component 9.20%, air-entraining component 5.00%, water-retaining component 0.10%, viscosity-increasing component 0.10% of water, 0.10% of anti-corrosion components and 85.50% of water;
[0062] Among them, the air-entraining component is composed of 57.14% by weight of sodium alkylbenzene sulfonate, 28.57% of sodium lauryl sulfate and 14.29% of triterpene saponins; the retarding component is composed of 83.34% by weight of glucose sodium tripolyphosphate, 8.33% white sugar and 8.33% sodium tripolyphosphate; the water-retaining component is composed of 50.00% hydroxypropyl methylcellulose and 50.00% sodium carboxymethyl cellulose; the antiseptic component is a compound Phenolics; the viscosity-enhancing component is polyethylene glycol.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com