A clear-faced concrete, high-strength technology, applied in the field of high-strength clear-faced concrete surface maintenance, can solve problems such as the inability to meet the long-term surface maintenance requirements of concrete, and achieve the effect of compact structure, good compression ratio and improved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] This embodiment relates to the surface maintenance method of high-strength fair-faced concrete. The weight components of each raw material of the maintenance material are: 90 parts of Portland cement, 30 parts of mineral powder, 15 parts of fly ash, 20 parts of ash calcium powder, 70 parts of quartz sand, 10 parts of wollastonite powder, 15 parts of polypropylene fiber, 15 parts of steel fiber, 3 parts of wood fiber, 20 parts of mortar enhancer and 100 parts of water.
[0018] The high-strength fair-faced concrete surface maintenance method involved in this embodiment includes:
[0019] (1) Preparation of high-strength fair-faced concrete surface maintenance materials: Weigh the weight components of Portland cement, mineral powder, fly ash, ash calcium powder, quartz sand, and wollastonite powder and send them to a high-speed twin-shaft mixer. Stir and mix for 5 to 7 minutes with a high-speed twin-shaft mixer at a rotational speed of 20 rpm to 30 rpm, add polypropylene ...
Embodiment 2
[0025] This embodiment is the same as the maintenance method in Embodiment 1, except that the weight components of each raw material of the maintenance material are: 150 parts of Portland cement, 50 parts of mineral powder, 25 parts of fly ash, 40 parts of ash calcium powder, quartz 100 parts of sand, 40 parts of wollastonite powder, 20 parts of polypropylene fiber, 20 parts of steel fiber, 5 parts of wood fiber, 50 parts of mortar enhancer and 200 parts of water.
[0026] The high-strength fair-faced concrete surface maintenance method involved in this embodiment has strong tensile performance and high compressive strength of the concrete surface.