Red tide inhibiting carbon powder and its prepn
A technology of charcoal powder and red tide, which is applied in the direction of botany equipment and methods, biocide, biocide, etc., can solve the problems of environmental re-pollution and high cost, and achieve the effect of improving the contact surface, simple production and long drug effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] The red tide suppressing and killing charcoal powder of the present invention is mainly prepared from the following raw materials in parts by weight:
[0029] 40g sawdust; 20g clay; 3g copper sulfate;
[0030] The preparation method of red tide suppressing and killing charcoal powder of the present invention comprises the following steps:
[0031] Molding: Take 40g of sawdust and 20g of clay according to the above parts by weight. After mixing, add 32g of water to the mixture. After the mixture is wet, put it into the molding equipment to make a block, and dry it to obtain the mixture A;
[0032] Carbonization: put the dried mixture A into the carbonization kiln, first heat it by dry distillation to make it burn initially, then seal the kiln door, leave it for the tuyere, slowly supply oxygen, and gradually increase the temperature to control the kiln temperature at 930 degrees , complete the carbonization to obtain the semi-finished product B.
[0033] Activation: Af...
Embodiment 2
[0036] The red tide suppressing and killing charcoal powder of the present invention is mainly prepared from the following raw materials in parts by weight:
[0037] Peanut skin 80g; clay 60g; copper sulfate 15g.
[0038] The preparation method of red tide suppressing and killing charcoal powder of the present invention comprises the following steps:
[0039] Molding: Take 80 g of peanut skins and 60 g of clay according to the above parts by weight. After mixing, add 9 g of water to the mixture. After the mixture is wet, put it into a molding equipment to make a block, and dry to obtain mixture A;
[0040] Carbonization: put the dried mixture A into the carbonization kiln, first heat it by dry distillation to make it burn initially, then seal the kiln door, leave it for the tuyere, slowly supply oxygen, and gradually increase the temperature to control the kiln temperature at 760 degrees , complete the carbonization to obtain the semi-finished product B.
[0041] Activation:...
Embodiment 3
[0044] The red tide suppressing and killing charcoal powder of the present invention is mainly prepared from the following raw materials in parts by weight:
[0045] Corn Cob 60; Clay 40; Copper Sulphate 9.
[0046] The preparation method of red tide suppressing and killing charcoal powder of the present invention comprises the following steps:
[0047] Molding: Take 60g of corncobs and 40g of clay according to the above parts by weight. After mixing, add 19g of water to the mixture. After the mixture is wet, put it into the molding equipment to make a block, and dry it to obtain the mixture A;
[0048] Carbonization: put the dried mixture A into the carbonization kiln, first heat it by dry distillation to make it burn initially, then seal the kiln door, leave it for the tuyere, slowly supply oxygen, and gradually increase the temperature to control the kiln temperature at 850 degrees , complete the carbonization to obtain the semi-finished product B.
[0049]Activation: Aft...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com