A technology of plastics and raw materials, applied in the direction of nails, staples, connecting components, etc., can solve the problems of plastic incompetence, no mention of plastic row nails, plastic nail performance can not meet the requirements of row nails, etc., to achieve simple molding , light weight, high strength effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Component weight parts ratio:
[0016] Nylon 6 50
[0017] Fiberglass 47
[0019] Y-(2,3-epoxypropoxy)propyltrimethoxysilane 0.4
[0020] Isopropyl tris (dioctyl pyrophosphate acyloxy) titanate 0.1
[0021] Tetrakis[β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionic acid]pentaerythritol ester 0.2
[0022] Tris(2,4-di-tert-butylphenyl)phosphite 0.2
[0024] 1) taking the above-mentioned various raw materials according to the ratio in parts by weight;
[0025] 2) Mix the above-mentioned raw materials in a mixer for 10 minutes;
[0026] 3) Put the mixed material into the twin-screw extruder, the glass fiber is added from the glass fiber inlet on the extruder, and then melted and extruded to granulate. The production process conditions are: temperature in zone 1-2 of the twin-screw extruder 240°C, 250°C for zone 3-4, 250°C for zone 5-6, 255°C for zone 7-8, 230°C for the head, and 300 rpm for the screw;
[0027] 4) After...
Embodiment 2
[0029] Component weight parts ratio:
[0030] Nylon 66 60
[0031] Fiberglass 30
[0033] Y-(2,3-epoxypropoxy)propyltrimethoxysilane 0.2
[0034] Isopropyl tris (dioctyl pyrophosphate acyloxy) titanate 0.2
[0035] N,N'-hexamethylenebis(3,5-di-tert-butyl-4-hydroxyphenylpropanamide) 0.3
[0036] Tris(2,4-di-tert-butylphenyl)phosphite 0.3
[0038] 1) taking the above-mentioned various raw materials according to the ratio in parts by weight;
[0039] 2) Mix the above-mentioned raw materials in a mixer for 10 minutes;
[0040] 3) Put the mixed material into the twin-screw extruder, the glass fiber is added from the glass fiber inlet on the extruder, and then melted and extruded to granulate. The production process conditions are: temperature in zone 1-2 of the twin-screw extruder The temperature is 240°C, the temperature in zone 3-4 is 255°C, the temperature in zone 5-6 is 265°C, the temperature in zone 7-8 is 260...
Embodiment 3
[0043] Component weight parts ratio:
[0044] Nylon 610 60
[0045] Fiberglass 35
[0046] mica 5
[0047] Y-(2,3-epoxypropoxy)propyltrimethoxysilane 0.3
[0048] Isopropyl tris (dioctyl pyrophosphate acyloxy) titanate 0.1
[0049] Tetrakis[β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionic acid]pentaerythritol ester 0.3
[0050] Tris(2,4-di-tert-butylphenyl)phosphite 0.3
[0051] N,N'-Ethylenebisstearamide 1
[0052] Operation process is with embodiment 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com