Recycling technology of polyhydroxyalkylphosphine and derivants thereof in leather tanning application
A technology of polyhydroxyalkylphosphine and hydroxyalkylphosphine, which is applied in the field of process technology and monitoring of effective substances in the recycling process of polyhydroxyalkylphosphine and its derivatives, can solve the problems of material waste and environmental damage, and achieve Low energy consumption, stable and consistent, easy-to-control effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Example 1: A technology for recycling polyhydroxyalkylphosphine and its derivatives in leather tanning applications
[0019] 1. Preparation of polyhydroxyalkylphosphine and its derivative tanning agent tanning initial solution:
[0020] In the initial tanning liquid, a mixture of stabilizer lauryl alcohol polyoxyethylene (9) ether (AEO-9), white sugar, pyrophosphate and preservatives was added, and its consumption was 0.1 of the pickling tare weight; the initial tanning liquid A mixture of buffering agent formic acid and sodium formate is added to the tanning solution, and its dosage is 3% of the pickling tare weight; the initial tanning liquid contains tetrakis hydroxymethyl phosphorus chloride and its polymer with urea, and the concentration is 1% of the pickling tare weight. %;
[0021] 2. Polyhydroxyalkylphosphine and its derivatives tanning agent cycle tanning applications:
[0022] Add pickled hides into the initial tanning solution, rotate for 360 minutes, add ...
Embodiment 2
[0024] Example 2: A technology for recycling polyhydroxyalkylphosphine and its derivatives in leather tanning applications
[0025] 1. Preparation of polyhydroxyalkylphosphine and its derivative tanning agent tanning initial solution:
[0026] A mixture of stabilizer lauryl alcohol polyoxyethylene (9) ether (AEO-9), polyvinyl alcohol, orthophosphorus salt and preservatives has been added to the initial tanning solution, and its consumption is 2% of the pickling tare weight A mixture of buffer formic acid and sodium formate is added to the initial tanning solution, and its consumption is 0.1% of the pickling tare weight; the initial tanning solution contains tetrahydroxypropyl phosphorus chloride and its polymer with urea, and the concentration is 5% of tare weight;
[0027] 2. Polyhydroxyalkylphosphine and its derivatives tanning agent cycle tanning applications:
[0028] Add pickled hides into the initial tanning solution, rotate for 90 minutes, add alkali in stages, and gr...
Embodiment 3
[0030] Example 3: A technology for recycling polyhydroxyalkylphosphine and its derivatives in leather tanning applications
[0031] 1. Preparation of polyhydroxyalkylphosphine and its derivative tanning agent tanning initial solution:
[0032] A mixture of stabilizer lauryl alcohol polyoxyethylene (9) ether (AEO-9), polyethanol, metaphosphate and preservatives was added to the initial tanning liquid, and the consumption was 1% of the pickling tare weight; A buffering agent is added to the initial tanning solution, and its dosage is 1.5% of the pickling tare weight; the initial tanning solution contains tetrahydroxyethyl phosphorus chloride and its polymer with urea, and the concentration is 3% of the pickling tare weight;
[0033] 2. Polyhydroxyalkylphosphine and its derivatives tanning agent cycle tanning applications:
[0034] Add pickled hides into the initial tanning solution, rotate for 230 minutes, add alkali in stages, and gradually increase the pH of the bath to 5-7. ...