Method for continuously preparing white carbon black and ammonium fluoride by carrying out fluosilicic acid ammoniation
A technology of white carbon black and fluorosilicic acid, which is applied in the field of preparing white carbon black and ammonium fluoride, can solve the problems of limited utilization of fluorine and silicon resources, small scale of a single set of equipment, and low utilization rate of equipment, and achieve shortening Effects of residence time, inhibition of agglomeration and hard agglomeration, and long operating cycle
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0022] When the temperature is 0°C and the compressed air is 0.2MPa, start stirring, and at the speed of 3000rpm, add 2% fluosilicic acid and 2% ammonia water at the same time, and the feed rates of fluosilicic acid and ammonia water are 80L / hr and 62L / hr respectively , the residence time is 30s, continuous reaction and filtration to obtain white carbon black filter cake and ammonium fluoride solution, the filter cake is washed and dried to obtain white carbon black. The main economic index of white carbon black within 24 hours is that the specific surface area is 320m2 / g; the DBP absorption value is 3.40, and the concentration of ammonium fluoride solution is 1.7%.
Embodiment 2
[0024] When the temperature is 15°C and the compressed air is 0.3MPa, start stirring, and at the speed of 8000rpm, add 15% fluosilicic acid and 15% ammonia water at the same time, and the feed rates of fluosilicic acid and ammonia water are 20L / hr and 16L / hr respectively , the residence time is 2min, continuous reaction and filtration to obtain white carbon black filter cake and ammonium fluoride solution, the filter cake is washed and dried to obtain white carbon black. The main economic index of white carbon black within 24 hours is that the specific surface area is 190m2 / g; the DBP absorption value is 2.80, and the concentration of ammonium fluoride solution is 13.7%.
Embodiment 3
[0026] When the temperature is 30°C and the compressed air is 0.4MPa, start stirring, and at the speed of 1000rpm, add 25% fluosilicic acid and 25% ammonia water at the same time, and the feeding amount of fluosilicic acid and ammonia water are 13.3L / hr and 10.3L respectively / hr, the residence time is 3min, continuously react and filter to obtain white carbon black filter cake and ammonium fluoride solution, and the filter cake is washed and dried to obtain white carbon black. The main economic index of white carbon black within 24 hours is that the specific surface area is 160m2 / g; the DBP absorption value is 2.20, and the concentration of ammonium fluoride solution is 23.9%.
PUM
Property | Measurement | Unit |
---|---|---|
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
specific surface area | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com