Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Fluoropolymer organic lining anticorrosive material for chimney, flue and other pipelines and containers and construction method thereof

A technology for anti-corrosion materials and chimneys, which can be used in anti-corrosion coatings, containers, combustion methods, etc., and can solve problems such as difficult construction.

Active Publication Date: 2010-11-24
重庆大众防腐股份有限公司
View PDF4 Cites 38 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0008] The purpose of the present invention is to solve the problems mentioned above in the technical application of existing fluorine rubber as anticorrosion materials, and to propose a polyfluorine organic lining anticorrosion material and construction method for chimneys, flues, other pipes and containers, which can be solved well. Fluorine rubber is difficult to construct as an anti-corrosion material. Realize that this type of material can be cured at room temperature and can be recoated many times to meet the anti-corrosion treatment needs of special fields such as chimneys and flues.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0054] In the present embodiment, polyfluorine organic (VP3-2, this is the code name given to this material by the applicant) organic lining anti-corrosion material is composed of A component and B component, wherein the compounded rubber for preparing A component consists of Parts ratio 100 parts fluorine content of 55% vinylidene fluoride / tetrafluoroethylene / hexafluoropropylene ternary fluororubber, 5 parts Ca(OH) 2 , 10 parts of MgO, 15 parts of carbon black, and 8 parts of bis-(4-aminohexylcyclohexyl) methane carbamate vulcanizing agent are mixed and prepared.

[0055] Prepare the putty type mortar of component A by slowly adding 100 parts of mixed rubber and 400 parts of acetone into the reaction kettle to dissolve the putty type mortar. The speed of the motor is controlled at 100 rpm, and finally A putty type glue for preparing the polyfluorine organic component A was obtained.

[0056] Component A consists of 100 parts by weight of putty type glue, 10 parts of 1mm-...

Embodiment 2

[0062] In this embodiment, polyfluorine organic (VP3-2) organic lining anticorrosion material is composed of A component and B component, wherein the compounded rubber for preparing A component is made of partial by weight ratio of 100 parts with a fluorine content of 60%. Fluoroethylene / tetrafluoroethylene / pentafluoropropylene ternary fluororubber, 5 parts of Ca(OH) 2 , 10 parts of MgO, 15 parts of calcium fluoride, and 8 parts of bis-(4-aminohexylcyclohexyl) methane carbamate vulcanizing agent.

[0063] All the other parts are the same as in Example 1.

Embodiment 3

[0065] In this example, the polyfluorine organic (VP3-2) lining anti-corrosion material is composed of A component and B component, wherein the compounded rubber for preparing A component is composed of metafluoride with a fluorine content of 65% by weight compared to 100 parts Ethylene / hexafluoropropylene binary fluororubber, 5 parts Ca(OH) 2 , 15 parts of MgO, and 20 parts of diatomaceous earth are mixed and made.

[0066] All the other parts are the same as in Example 1.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides an anticorrosive material for a chimney, a flue and other containers and pipelines and an anticorrosive construction process. The construction method of the anticorrosive material comprises the following steps: using crude rubber with higher fluorine content as a raw material, then adding curing agent, stabilizer, special stuffing and other components, and mixing to form precuring gross rubber; dissolving the rubber by using low-molecular weight esters and ketones as the solvent to form a putty type rubber paste; and finally, adding special additives, uniformly mixing, coating to the inner walls of a chimney, a flue and a chemical container, and curing into the polymerized fluororubber organic lining under the room-temperature condition. The material can be independently used as the anticorrosive material, and can also be used for protecting common foam glass bricks (ceramic bricks) and adhesive for anticorrosive purpose in the domestic chimney (flue) at present. The invention well solves the technical problems of fluororubber room-temperature curing and difficult anticorrosive construction, can be used in a high-temperature environment of more than 230 DEG C, and can endure high-concentration sulfuric acid, nitric acid, hydrochloric acid, phosphoric acid, hydrofluoric acid, corresponding salts and a mixture thereof. The anticorrosive lining material is economically affordable, has extremely high comprehensive anticorrosive properties such as temperature resistance, acid resistance and the like, and is applicable to the anticorrosive treatment of a cured chimney.

Description

technical field [0001] The invention relates to an anti-corrosion lining material with high temperature resistance and strong corrosion resistance and an application process. It is mainly used in the anti-corrosion of chimneys and flues after desulfurization in thermal power plants, and can also be used in containers and containers involved in petroleum, chemical and metallurgy. The anticorrosion of the inner wall of the pipeline belongs to the field of organic polymer materials. Background technique [0002] At present, there are gaps or insufficient experience in anti-corrosion measures for chimneys after desulfurization, whether in terms of chimney design, construction and other standard specifications, or in practical engineering applications. Due to investment and technical problems, the five major power plants in my country Led by the group, since the second half of 2006, 80% of the start-up projects of various power generation companies have adopted the removal of the ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D127/16C09D127/20C09D127/12C09D127/18C09D123/14C09D7/12C09D5/08F23J13/02F16L58/10B65D90/04B65D23/02B65D25/14
CPCY02W90/10
Inventor 杨祖洪
Owner 重庆大众防腐股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products