Method for slime fluidized bed boiler desulphurization of sludge and white slime of papermaking factory
A technology for fluidized bed boilers and paper mills, applied in chemical instruments and methods, sludge treatment, water/sludge/sewage treatment, etc., to achieve cost savings, save the link of sulfur removal, and save costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0039]For a 65-ton coal slime fluidized bed boiler, the coal slime conveyor transports about 18 tons of coal slurry per hour, and the sulfur content is 0.5% after testing; the temperature of the coal slime fluidized bed boiler is 850 degrees. The water content of the white mud produced by the paper mill is 55%, and the calcium carbonate content in the solid white mud is detected to be 95%. The sludge produced by the paper mill has a water content of 70%, and the sludge in the solid state contains 50% calcium oxide.
[0040] The sludge is transported to the dehydration workshop by means of transportation, and the sewage is pressurized by the air, and the pressure is 1.4MPa to remove the water content to 65%, and then use mechanical pressure to remove the water content of the sludge to 55%. Transport the white mud to the dog chemical workshop, wash with water, remove impurities with a diameter greater than 8cm in the white mud, and dehydrate the white mud with a pre-hanging filt...
Embodiment 2
[0042] For a 210-ton coal slime fluidized bed boiler, the coal slime conveyor transports about 60 tons of coal slurry per hour, and the sulfur content is 1% after testing; the temperature of the coal slime fluidized bed boiler is 880 degrees. The white mud produced by the paper mill has a water content of 50%, and the calcium carbonate content in the solid white mud is detected to be 90%. The sludge produced by the paper mill has a water content of 75%, and the sludge in the solid state contains 55% of calcium oxide.
[0043] The sludge is transported to the dehydration workshop by means of transportation, and the sewage is pressurized by air at a pressure of 1.5MPa to remove the water content to 60%, and then use mechanical pressure to remove the water content of the sludge to 50%. Transport the white mud to the dog chemical workshop, wash with water, remove impurities with a diameter greater than 8cm in the white mud, and dehydrate the white mud with a pre-hanging filter, so...
Embodiment 3
[0045] For a 140-ton coal slime fluidized bed boiler, the coal slime conveyor transports about 40 tons of coal slurry per hour, and the sulfur content is 0.8% after testing; the temperature of the coal slime fluidized bed boiler is 900 degrees. The water content of the white mud produced by the paper mill is 52%, and the calcium carbonate content in the solid white mud is detected to be 96%. The sludge produced by the paper mill has a water content of 73%, and the sludge in the solid state contains 52% of calcium oxide.
[0046] The sludge is transported to the dehydration workshop by means of transportation, and the sewage is pressurized by the air, and the pressure is 1.6MPa to remove the water content to 58%, and then use mechanical pressure to remove the water content of the sludge to 52%. Transport the white mud to the dog chemical workshop, wash with water, remove impurities with a diameter greater than 8cm in the white mud, and dehydrate the white mud with a pre-hanging...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com