Preparation method for aqueous floor coating

A floor coating, water-based technology, applied in the field of coating materials, can solve problems such as damage, and achieve the effect of avoiding pollution, avoiding personal health, and meeting environmental protection requirements

Inactive Publication Date: 2014-04-09
张锦碧
View PDF6 Cites 10 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] The present invention adopts water-based epoxy curing agent, auxiliary agent, defoamer, quartz powder, precipitated barium sulfate, thickener, liquid epoxy resin, active diluent, and environment-friendly organic solvent to prepare a kind of water-based floor coating. Water-based floor coatings can avoid environmental pollution, avoid damage to human health, have strong air permeability, are suitable for use on wet base surfaces, and meet environmental protection requirements. Related patents have not yet been applied in China

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] A kind of water-based floor paint, this water-based floor paint is made up of A, B two components, and the parts by weight of each component are:

[0026] 85 parts of component A, 44 parts of component B; the raw material ratio of component A is: 32 parts of water, 18 parts of water-based epoxy curing agent, 1.2 parts of auxiliary agent, 0.2 parts of defoaming agent, and 11 parts of quartz powder , 6 parts of precipitated barium sulfate, 0.3 parts of thickener, the raw material ratio of component B is: 15 parts of liquid epoxy resin, 1.3 parts of reactive diluent, and 3.3 parts of environmentally friendly organic solvent.

[0027]

[0028] A kind of preparation method of waterborne floor coating, its preparation process comprises:

[0029] After dispersing the raw materials of component A at 1200rpm for 5-10 minutes at a high speed, grind them through a sand mill to a fineness of 13um, add the remaining water and mix at 600rpm for 7 minutes to obtain component A, and m...

Embodiment 2

[0031] A kind of water-based floor paint, this water-based floor paint is made up of A, B two components, and the parts by weight of each component are:

[0032] 98 parts of component A, 48 parts of component B; the raw material ratio of component A is: 34 parts of water, 24 parts of water-based epoxy curing agent, 2.6 parts of auxiliary agent, 0.5 part of defoamer, and 13 parts of quartz powder , 9 parts of precipitated barium sulfate, 0.7 parts of thickener, the raw material ratio of component B is: 17.5 parts of liquid epoxy resin, 2.2 parts of reactive diluent, and 3.6 parts of environmentally friendly organic solvent.

[0033]

[0034] A kind of preparation method of waterborne floor coating, its preparation process comprises:

[0035] After dispersing the raw materials of component A at 1300rpm for 8 minutes at high speed, grind them through a sand mill to a fineness of 25um, add the remaining water and mix at 650rpm for 8 minutes to obtain component A, and mix the raw ...

Embodiment 3

[0037] A kind of water-based floor paint, this water-based floor paint is made up of A, B two components, and the parts by weight of each component are:

[0038] 88 parts of component A, 48 parts of component B; the raw material ratio of the component A is: 33 parts of water, 22 parts of water-based epoxy curing agent, 2 parts of auxiliary agent, 0.5 part of defoamer, and 13 parts of quartz powder , 7 parts of precipitated barium sulfate, 0.4 parts of thickener, the raw material ratio of component B is: 16 parts of liquid epoxy resin, 2 parts of reactive diluent, and 3.7 parts of environmentally friendly organic solvent.

[0039] A kind of preparation method of waterborne floor coating, its preparation process comprises:

[0040] After dispersing the raw materials of component A at 1500rpm for 8 minutes at high speed, grind them through a sand mill to a fineness of 27um, add the remaining water and mix at 680rpm for 9 minutes to obtain component A, and mix the raw materials of...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to a preparation method for an aqueous floor coating. The aqueous floor coating is prepared from the components in parts by weight of 80-100 parts of a component A and 40-50 parts of a component B, wherein the component A is prepared from the following components in parts by weight of 30-35 parts of water, 15-25 parts of an aqueous epoxy curing agent, 1-3 parts of an adjuvant, 0.1-0.7 part of an antifoaming agent, 10-15 parts of quartz powder, 5-10 parts of precipitated barium sulfate and 0.2-0.8 part of a thickening agent; the component B is prepared from the following raw materials in parts by weight of 15-18 parts of liquid epoxy resin, 1-3 parts of a reactive diluent and 3-4 parts of an environment-friendly type organic solvent. The preparation method comprises the following steps: dispersing the raw materials of the component A at a high speed of 1000-2000rpm for 5-10 minutes; grinding the raw materials of the component A until the fitness is 10-30 microns; mixing the raw materials with the residual water at a speed of 500-800rpm for 3-10 minutes, so as to obtain the component A; mixing the raw materials of the component B at a speed of 200-600rpm for 10-20 minutes, so as to obtain the component B; mixing the component A and the component B at a ratio ranging from 1:1 to 1:3, so as to obtain the aqueous floor coating. The aqueous floor coating can avoid the environment pollution and damage on human health, has strong air permeability, is applicable to wet basal plane, and meets the requirements on the environmental friendliness.

Description

technical field [0001] The invention relates to a method for preparing a water-based floor coating, in particular to a water-based floor coating that can avoid environmental pollution, avoid damage to personal health, has strong air permeability, is suitable for use on wet base surfaces, and meets environmental protection requirements, and belongs to coatings material field. Background technique [0002] Modern industry has put forward more and more stringent requirements on the floor. For example, food, medicine and other industries require the floor to be dust-free, free of harmful volatiles, and clean and dust-free; the machinery industry requires strong mechanical shock resistance, wear resistance, and It has been rolled by forklifts and other vehicles for a long time, and it is easy to repair even if it is partially damaged; the ground of industrial workshops such as machine tools and instruments is often corroded and leaked by various oils, which is difficult to comple...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D163/00C09D7/12
Inventor 张锦碧
Owner 张锦碧
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products