Recycling technology for manufacturing industrial pallets by utilizing organic solid waste in furniture industry
A solid waste and pallet technology, applied in the field of solid waste recycling of industrial pallets, can solve the problems of quality impact, increased fragmentation of finished products, high cost, etc., achieve good molding performance, improve impact resistance, and reduce crushing costs Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0070] The first step is to prepare modified wood material powder
[0071] Collect woody solid waste from the furniture industry and crush it into 10-1000 mesh waste woody material powder. The prepared modified woody material powder contains:
[0072]100 kg of waste wood material powder, 10-13 kg of nano-scale calcium carbonate and / or nano-scale calcium sulfate (the average particle size of both is 10-100nm), 2-2.5 kg of titanate coupling agent, 5-6 kg of silicone oil kg, 0.8-1.2 kg of stearic acid.
[0073] The above-mentioned nano-scale calcium carbonate or / and calcium sulfate and the waste wood material powder that has been dried in a fluidized furnace and controlled to keep the moisture below 3% are vigorously stirred in a high-speed mixer at 1200-1500 rpm and 90-110°C for 20 minutes. Minutes, then add titanate coupling agent, stearic acid, silicone oil and continue mixing for 6-8 minutes to obtain modified wood material powder.
[0074] The second step is to prepare the...
Embodiment 2
[0083] Collect wood solid waste from the furniture industry, crush it into 10-100 mesh (abbreviated as: waste wood material powder in the present invention), and prepare modified wood material powder according to the following ratio:
[0084] 100-150 kg of waste wood material powder, 20-27 kg of nanoscale calcium carbonate and / or nanoscale calcium sulfate (the average particle size of both is 10-100nm), 3-6 kg of titanate coupling agent, stearin 1-2.5 kg of acid, 5-9 kg of silicone oil.
[0085] Stir 50% of the above-mentioned nano-scale carbonic acid and / or nano-scale calcium sulfate with the waste wood material powder whose water content is controlled below 2% after drying in a high-speed mixer for 12-20 minutes, and then add titanate coupler The joint agent, stearic acid and silicone oil continue to mix for 7-10 minutes and then add the following substances:
[0086] The remaining 50% of nano-scale calcium carbonate and / or nano-scale calcium sulfate, 8-10 kg of ultra-fine ...
Embodiment 3
[0091] Use sawdust, crop stalks, rice bran, other plant stems and leaves, paper, etc. to replace the waste woody material powder, or their mixture, and refer to Example 1 or 2 for other methods.
[0092]
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com