High-fastness and environment-friendly wood board processing process
A processing technology and wood board technology, applied in the direction of wood processing appliances, wood veneer joining, manufacturing tools, etc., can solve the problems of high release of free formaldehyde in finished products, damage to the legitimate rights and interests of consumers, and impact on the quality of board processing, etc. Achieve the effect of not easy to bend and deform, low manufacturing cost and high production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] A kind of strong fastness and environment-friendly woodworking board processing technology is characterized in that, described processing technology comprises the following steps:
[0020] (1) Pretreatment of raw materials: Soak the wood in water for 6 days, with a moisture content of more than 40%, and then boil it in water at a temperature of 110°C for 2.5 hours. day, make the moisture content be 12-13%, and use a planer to plan a square material with a thickness of 10cm;
[0021] (2) Wooden core board: Paste the veneer with a layer of oak veneer, then glue it and paste it with a layer of skin, press it with a hot pressing block with a temperature of 1000°C for 4 minutes, and flatten it up and down on a cold press Press for 10h;
[0022] (3) Glue preparation: according to the weight distribution ratio as follows: 100 parts of low-formaldehyde urea-formaldehyde resin, 25 parts of bentonite, and 0.5 part of vinyl triamine, the above-mentioned raw materials are stirred ...
Embodiment 2
[0025] A kind of strong fastness and environment-friendly woodworking board processing technology is characterized in that, described processing technology comprises the following steps:
[0026] (1) Pretreatment of raw materials: Soak the wood in water for 7 days, with a moisture content of more than 40%, and then boil it in water at 120°C for 2 hours. When the temperature drops to 70°C, enter the drying kiln and dry at 110°C for 3 days. , so that the water content is 12-13%, planed into a 10cm thick square with a planer;
[0027] (2) Wooden core board: Paste the veneer with a layer of oak veneer, then glue it and paste it with a layer of skin, press it with a hot pressing block with a temperature of 1000 ° C for 5 minutes, and flatten it up and down on a cold press Press 9h;
[0028] (3) Glue preparation: according to the weight distribution ratio as follows: 100 parts of low-formaldehyde urea-formaldehyde resin, 25 parts of diatomaceous earth, 0.6 part of diaminodiphenyl s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com