Efficient fuel-coal sulfur-fixation agent based on oyster shells and preparation method
A technology of oyster shells and sulfur-fixing agents, applied in the direction of fuel, solid fuel, petroleum industry, etc., can solve problems such as endangering residents' lives, corruption and odor, and environmental pollution, so as to increase residence time, improve sulfur-fixing reactions, and reduce The effect of sulfur fixation costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A high-efficiency coal-burning sulfur-fixing agent based on oyster shells, including the following raw materials in parts by weight: nano-active titanium dioxide 12, oyster shells 70, porous silicon nitride 14, combustion aid potassium nitrate 3.5, strengthening agent potassium permanganate 4.5, Oxidation catalyst manganese oxalate 4, stabilizer sodium tartrate 22, dispersant liquid paraffin 9.5, sodium alkylbenzene sulfonate 9, appropriate amount of deionized water.
[0017] A preparation method based on an efficient coal-burning sulfur-fixing agent of oyster shells, comprising the following steps:
[0018] (1) Put the oyster shells into a pulverizer and pulverize for 3.5 hours, pass through 100 meshes to obtain superfine powder of oyster shells, mix nano-active titanium dioxide, porous silicon nitride, dispersant liquid paraffin, and superfine powders of oyster shells, and stir at a high speed first , and then calcined at 600°C for 2.5 hours at a high temperature to o...
Embodiment 2
[0023] A high-efficiency coal-burning sulfur-fixing agent based on oyster shells, including the following raw materials in parts by weight: nano-active titanium dioxide 11, oyster shells 75, porous silicon nitride 13, combustion aid potassium nitrate 3.5, strengthening agent potassium permanganate 4.5, Oxidation catalyst manganese oxalate 4, stabilizer sodium tartrate 22, dispersant liquid paraffin 9.5, sodium alkylbenzene sulfonate 9, appropriate amount of deionized water.
[0024] A preparation method based on an efficient coal-burning sulfur-fixing agent of oyster shells, comprising the following steps:
[0025] (1) Put the oyster shells into a pulverizer and pulverize for 3.5 hours, pass through 100 meshes to obtain superfine powder of oyster shells, mix nano-active titanium dioxide, porous silicon nitride, dispersant liquid paraffin, and superfine powders of oyster shells, and stir at a high speed first , and then calcined at 600°C for 2.5 hours at a high temperature to o...
Embodiment 3
[0030] A high-efficiency coal-burning sulfur-fixing agent based on oyster shells, including the following raw materials in parts by weight: nano-active titanium dioxide 10, oyster shells 80, porous silicon nitride 12, combustion aid potassium nitrate 3.5, strengthening agent potassium permanganate 4.5, Oxidation catalyst manganese oxalate 4, stabilizer sodium tartrate 22, dispersant liquid paraffin 9.5, sodium alkylbenzene sulfonate 9, appropriate amount of deionized water.
[0031] A preparation method based on an efficient coal-burning sulfur-fixing agent of oyster shells, comprising the following steps:
[0032] (1) Put the oyster shells into a pulverizer and pulverize for 3.5 hours, pass through 100 meshes to obtain superfine powder of oyster shells, mix nano-active titanium dioxide, porous silicon nitride, dispersant liquid paraffin, and superfine powders of oyster shells, and stir at a high speed first , and then calcined at 600°C for 2.5 hours at a high temperature to o...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com