[0059] In one embodiment of the present invention, the heat exchange pool 2003 is a sealed pressure vessel, and a control valve 6000 is respectively provided on the water inlet pipe 2001 and the water outlet pipe 2002, and a pressurizing device 9000 is provided outside the pond 1000, The pressurization device 9000 is connected to the heat exchange tank 2003 through a pressurization pipe 9001, and a control valve 6000 is provided on the pressurization pipe 9001.
[0060] In the present invention, an anti-rust coating is provided on the outside of the storage tank 2, and the anti-rust coating includes the following components by weight percentage:
[0061]
[0062] Preparation method: Mix and stir graphene, strontium chromate, trilead tetroxide, ammonium metaborate, and titanium dioxide evenly, grind in a conical grinder until the fineness is <60 μm, then add silicone modified acrylate emulsion, o- Dibutyl phthalate, propylene glycol methyl ether and other components are unif...
Embodiment 4
[0082] Example 4 - Corrosion Resistant Coating
[0083] Corrosion-resistant coatings include the following components by weight percentage:
[0084]
[0085] Preparation method: Mix fluorinated acrylate and coal tar pitch evenly, stir and heat to 45°C, stir for 10 minutes, add nepheline powder and zinc citrate, heat to 120°C, stir for 3 hours, cool to 50°C, add other components , stirred and kept for 1 hour, ultrasonically dispersed for 10 minutes, and ground to a fineness of <60 μm in a conical grinder.
Embodiment 5
[0086] Example 5 - Corrosion Resistant Coating
[0087] Corrosion-resistant coatings include the following components by weight percentage:
[0088]
[0089] Preparation method: Mix fluorinated acrylate and coal tar pitch evenly, stir and heat to 60°C, stir for 60 minutes, add nepheline powder and zinc citrate, heat to 145°C, stir for 5 hours, cool to 60°C, add other components , stirred and kept for 2 hours, ultrasonically dispersed for 25 minutes, and ground to a fineness of <60 μm in a conical grinder.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com