Preparation method of calcium alginate microspheres with core-shell structure
A calcium alginate and core-shell structure technology, applied in the field of polymer microsphere preparation, can solve the problems of poor biocompatibility of materials, complicated preparation methods, and limited development, and achieve good stability, high mechanical strength, and easy operating conditions The effect of control
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0025] First, mix 100 parts of polyvinyl alcohol solution (10%) and 90 parts of sodium alginate solution (10%) to form a uniform mixture, then add 200 parts of the load into the above mixture until a uniform mixture is formed . Then, the above mixture is continuously added dropwise into 9% borax aqueous solution to form microspheres with a diameter of about 4mm. Finally, the above-mentioned microspheres are taken out, and the microspheres are added to 10% calcium chloride solution again under stirring conditions, so that the surface of the above-mentioned microspheres forms a calcium alginate coating layer, and calcium alginate with a core-shell structure can be obtained. Microspheres.
example 2
[0027] First, mix 100 parts of polyvinyl alcohol solution (10%) and 100 parts of sodium alginate solution (10%) to form a uniform mixture, then add 180 parts of the load into the above mixture until a uniform mixture is formed . Then, the above mixture is continuously added dropwise into 10% borax aqueous solution to form microspheres with a diameter of about 4mm. Finally, the above-mentioned microspheres are taken out, and the microspheres are added to 8% calcium chloride solution again under stirring conditions, so that the surface of the above-mentioned microspheres forms a calcium alginate coating layer, and calcium alginate with a core-shell structure can be obtained. Microspheres.
example 3
[0029] First, mix 100 parts of polyvinyl alcohol solution (10%) and 110 parts of sodium alginate solution (8%) to form a uniform mixture, then add 150 parts of the load into the above mixture until a uniform mixture is formed . Then, the above mixture was continuously added dropwise into 8% borax aqueous solution to form microspheres with a diameter of 3 mm. Finally, the above-mentioned microspheres are taken out, and the microspheres are added to 6% calcium chloride solution again under stirring conditions, so that the surface of the above-mentioned microspheres forms a calcium alginate coating layer, and calcium alginate with a core-shell structure can be obtained. Microspheres.
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Diameter | aaaaa | aaaaa |
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com