A technology for alkylating acid hydrocarbons and coalescing fillers. It is used in immiscible liquid separation, chemical/physical processes, chemical instruments and methods. It can solve problems such as poor separation effect, achieve rational utilization of resources and excellent acid resistance Good performance and processability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] (1) Add 10 parts of polyvinyl acetate and 8 parts of polyethylene terephthalate to 25 parts of ultra-fine polytetrafluoroethylene powders, mix well and then microwave at microwave frequency 2450MHz and power 700W for 5min, then Add 4 parts of hydrogenated rosin glyceride and 3 parts of petroleum coke powder, mix well, and continue microwave treatment for 3 minutes to obtain material I;
[0015] (2) Add 8 parts of linear low density polyethylene and 4 parts of polyvinyl butyral to 10 parts of powdered chloroprene rubber, mix well, and microwave at microwave frequency 2450MHz, power 700W for 5min, then add 2 parts while hot Epoxidized soybean oil, 2 parts of nano rubber powder and 0.5 part of nano graphite powder are mixed evenly to obtain material II;
[0016] (3) Add material II, 5 parts of volcanic ash, 8 parts of activated clay, 3 parts of ceramic micropowder and 2 parts of asbestos wool to material I, heat to 100-110°C and mix for 10 minutes, then add 3 parts of cety...
Embodiment 2
[0018] (1) Add 10 parts of polyvinyl acetate and 10 parts of polyethylene terephthalate to 30 parts of ultra-fine polytetrafluoroethylene powder, mix well and then microwave at microwave frequency 2450MHz, power 700W for 5min, then Add 4 parts of hydrogenated rosin glyceride and 3 parts of petroleum coke powder, mix well, and continue microwave treatment for 3 minutes to obtain material I;
[0019] (2) Add 6 parts of linear low density polyethylene and 4 parts of polyvinyl butyral to 10 parts of powdered chloroprene rubber, mix well, and microwave at microwave frequency 2450MHz, power 700W for 5min, then add 2 parts while hot Epoxidized soybean oil, 1 part of nano rubber powder and 1 part of nano graphite powder are mixed evenly to obtain material II;
[0020] (3) Add material II, 8 parts of volcanic ash, 5 parts of activated clay, 5 parts of ceramic micropowder and 3 parts of asbestos wool to material I, and heat to 100-110 ° C for 10 minutes, then add 2 parts of cetyl alcoho...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com