A technology of equipment and thermal insulation protection, applied in the field of machinery, can solve the problems of mvr equipment not having thermal insulation, easy damage of mvr equipment, increasing equipment scrapping rate, etc., achieving good dispersion effect, increasing lifespan and reducing scrapping rate.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] This embodiment provides a heat-insulating MVR device and its preparation method. The MVR device is coated with a layer of heat-insulating protective layer. The heat-insulating protective layer is composed of two components, A and B, in a ratio of A:B=2:1. A and B comprise the following components in parts by mass:
[0031] Component A includes the following components in parts by mass: 32 parts of ATO powder, 27 parts of alcohol-soluble acrylic resin, 9 parts of ethanol, 12 parts of dispersant, 8 parts of leveling agent, and thickener: 5 parts, UV absorber: 9 parts, sodium tetraborate: 3 parts, potassium hydrogen phthalate: 4 parts;
[0032] Component B includes the following components in parts by mass: defoamer: 11 parts, mixed phosphate: 2 parts, styrene-butadiene rubber: 13 parts, silicon dioxide: 11 parts, flame retardant: 9 parts, auxiliary materials : 3 parts, polyphenylene ether resin powder: 18 parts, water: 44 parts;
[0033] Among them, the alcohol-soluble...
Embodiment 2
[0040] This embodiment provides a heat-insulating MVR device and its preparation method. The MVR device is coated with a layer of heat-insulating protective layer. The heat-insulating protective layer is composed of two components, A and B, in a ratio of A:B=2:1. A and B comprise the following components in parts by mass:
[0041] Component A includes the following components in parts by mass: 36 parts of ATO powder, 33 parts of alcohol-soluble acrylic resin, 13 parts of ethanol, 16 parts of dispersant, 13 parts of leveling agent, and thickener: 7 parts, UV absorber: 13 parts, sodium tetraborate: 6 parts, potassium hydrogen phthalate: 8 parts;
[0042] Component B includes the following components in parts by mass: defoamer: 16 parts, mixed phosphate: 5 parts, styrene-butadiene rubber: 16 parts, silicon dioxide: 14 parts, flame retardant: 15 parts, auxiliary materials : 6 parts, polyphenylene ether resin powder: 24 parts, water: 48 parts;
[0043] Among them, the alcohol-sol...
Embodiment 3
[0050] This embodiment provides a heat-insulating MVR device and its preparation method. The MVR device is coated with a heat-insulating protective layer, and the heat-insulating protective layer is composed of two components, A and B, in a ratio of A:B=2:1. A and B comprise the following components in parts by mass:
[0051] Component A includes the following components in parts by mass: 34 parts of ATO powder, 30 parts of alcohol-soluble acrylic resin, 11 parts of ethanol, 14 parts of dispersant, 10 parts of leveling agent, and thickener: 6 parts, UV absorber: 11 parts, sodium tetraborate: 5 parts, potassium hydrogen phthalate: 6 parts;
[0052] Component B includes the following components in parts by mass: defoamer: 14 parts, mixed phosphate: 4 parts, styrene-butadiene rubber: 14 parts, silicon dioxide: 13 parts, flame retardant: 14 parts, auxiliary materials : 5 parts, polyphenylene ether resin powder: 22 parts, water: 46 parts;
[0053] Wherein, the alcohol-soluble acr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com