Power cable with excellent mechanical performances
A power cable and mechanical technology, applied in the field of power cables, can solve the problems of insulation resistance and breakdown voltage drop, easy breeding of bacteria to corrode the sheath layer, and shorten the service life of the cable, so as to achieve good bonding adjustment, enhanced toughness, The effect of water resistance enhancement
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A power cable with excellent mechanical properties proposed by the present invention includes a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 38 parts of ethylene-vinyl acetate polymer, chlorinated polyethylene 40 parts, 1.5 parts of tricresyl phosphate, 2 parts of microcrystalline paraffin, 24 parts of diatomite, 10 parts of sepiolite powder, 45 parts of white carbon black, 17 parts of glass beads, 4 parts of wollastonite, 30 parts of modified bentonite 3 parts of zinc oxide, 0.8 parts of triallyl isocyanurate, 0.4 parts of cyclohexanone peroxide, 1.6 parts of benzoyl peroxide, 0.5 parts of anti-aging agent AW, and 2.5 parts of anti-aging agent NBC.
Embodiment 2
[0018] A power cable with excellent mechanical properties proposed by the present invention includes a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 48 parts of ethylene-vinyl acetate polymer, chlorinated polyethylene 30 parts, 2.5 parts of tricresyl phosphate, 1 part of microcrystalline paraffin, 32 parts of diatomite, 6 parts of sepiolite powder, 65 parts of white carbon black, 13 parts of glass microspheres, 10 parts of wollastonite, 20 parts of modified bentonite 5 parts of zinc oxide, 0.4 parts of triallyl isocyanurate, 1 part of cyclohexanone peroxide, 0.8 parts of benzoyl peroxide, 1 part of anti-aging agent AW, and 1.5 parts of anti-aging agent NBC.
[0019] The modified bentonite in the raw material of the sheath layer is prepared by the following process: mix and stir lauryl amidopropyl betaine and water, add copper sulfate solution dropwise, stir after the addition is complete, and use so...
Embodiment 3
[0021] A power cable with excellent mechanical properties proposed by the present invention includes a conductor and a sheath layer coated on the outside of the conductor; the raw materials of the sheath layer include by weight: 40 parts of ethylene-vinyl acetate polymer, chlorinated polyethylene 38 parts, 1.8 parts of tricresyl phosphate, 1.6 parts of microcrystalline paraffin, 26 parts of diatomite, 9 parts of sepiolite powder, 50 parts of white carbon black, 16 parts of glass beads, 5 parts of wollastonite, 28 parts of modified bentonite 3.5 parts of zinc oxide, 0.7 parts of triallyl isocyanurate, 0.6 parts of cyclohexanone peroxide, 1.4 parts of benzoyl peroxide, 0.6 parts of anti-aging agent AW, and 2.2 parts of anti-aging agent NBC.
[0022] The modified bentonite in the raw material of the sheath layer is prepared by the following process: 6 parts by weight of lauryl amidopropyl betaine and 45 parts of water are mixed and stirred for 30 minutes, and 4 parts of copper sul...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com