A printing and packaging and plasticizer technology, applied in the field of degradable and easy-to-print packaging films and packaging films, can solve the problems of poor transparency and dryness, contradictions of wood pulp and paper resources, and inability to meet various packaging industries, so as to improve transparency , Excellent printability, smooth and dry film surface effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A degradable and easy-to-print packaging film is prepared from the following raw materials in parts by mass
[0024] 100 parts of PVC resin,
[0025] Phosphoric acid diester 5 parts,
[0026] 2 parts barium stearate and zinc stearate mixture,
[0027] 0.5 part of fatty acid ester,
[0028] 1 part softener,
[0029] Silicone-fatty acid ester compound 6 parts, (not only helps to improve transparency, but also can obtain a smooth and dry film surface, so that the film has excellent printability)
[0030] Polylactic acid 10 parts
[0031] 1.5 parts of sodium n-hexadecyl sulfate (surface modifier, maintain the clarity of the film).
Embodiment 2
[0033] A degradable and easy-to-print packaging film is prepared from the following raw materials in parts by mass
[0034] 100 parts of PVC resin,
[0035] 7 parts of ethylene glycol phosphite,
[0036] Chromium stearate and calcium stearate mixture 2 parts,
[0037] Fatty amide 2 parts,
[0038] Softener 2 parts,
[0039] Silicone-fatty acid ester compound 7 parts, (not only helps to improve transparency, but also can obtain a smooth and dry film surface, so that the film has excellent printability)
[0040] Polylactic acid 13 parts
[0041] 3 parts of sodium n-hexadecyl sulfate (surface modifier, maintain the clarity of the film).
Embodiment 3
[0043] A degradable and easy-to-print packaging film is prepared from the following raw materials in parts by mass
[0044] 100 parts of PVC resin,
[0045] 8 parts of triethyl phosphate,
[0046] 3 parts zinc stearate and chromium stearate mixture,
[0047] 4 parts polyethylene wax,
[0048] 3 parts softener,
[0049] Silicone-fatty acid ester compound 8 parts, (not only helps to improve transparency, but also can obtain a smooth and dry film surface, so that the film has excellent printability)
[0050] Polylactic acid 15 parts
[0051] 5 parts of sodium n-hexadecyl sulfate (surface modifier, maintain the clarity of the film).