High-performance air filter paper and preparation method and application thereof
An air filter paper, modified technology, applied in the field of filter paper, can solve the problems of filtration efficiency lower than 90%, paper deformation, high tightness, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0032] Air filter paper, including base paper and an impregnating agent for impregnating the base paper, the fibers used in the base paper include 20 parts by weight of high-density cotton linter pulp, 5 parts of polypropylene fiber, and alkali-free glass fiber chopped strands 20 parts, 3 parts of ceramic fiber and 10 parts of carbon fiber, 0.1 part of amphoteric polyacrylamide used in base paper preparation, 0.2 part of modified starch light calcium carbonate, 0.5 part of polyethylene oxide with a molecular weight of 2.5 million to 3 million.
[0033] The preparation of the high-density cotton linter pulp is obtained by adding YY-02 penetrating agent for beating and then alkali cooking.
[0034] The alkali-free glass fiber chopped strands are produced by the following method: firstly, the alkali-free glass balls are heated to 1600-1800°C to melt, then the molten alkali-free glass balls are sprayed to obtain glass fibers, and finally the obtained glass fibers are cut to obtain ...
Embodiment 2
[0050] Air filter paper, including base paper and an impregnating agent for impregnating the base paper, the fibers used in the base paper include 40 parts by weight of high-density cotton linter pulp, 12 parts of polypropylene fiber, and alkali-free glass fiber chopped strands 40 parts, 8 parts of ceramic fiber and 20 parts of carbon fiber, 4 parts of amphoteric polyacrylamide used in the preparation of base paper, 0.8 part of modified starch light calcium carbonate, 5 parts of polyethylene oxide with a molecular weight of 2.5 million to 3 million, defoaming 0.2 parts of the agent.
[0051] The preparation of the high-density cotton linter pulp is obtained by adding YY-02 penetrating agent for beating and then alkali cooking.
[0052] The alkali-free glass fiber chopped strands are produced by the following method: firstly, the alkali-free glass balls are heated to 1600-1800°C to melt, then the molten alkali-free glass balls are sprayed to obtain glass fibers, and finally the...
Embodiment 3
[0068] Air filter paper, including base paper and an impregnating agent for impregnating the base paper, the fibers used in the base paper include 30 parts by weight of high-density cotton linter pulp, 10 parts of polypropylene fiber, and alkali-free glass fiber chopped strands 35 parts, 6 parts of ceramic fiber and 15 parts of carbon fiber 2.5 parts of amphoteric polyacrylamide, 0.4 part of modified starch light calcium carbonate, 2.5 parts of polyethylene oxide with molecular weight of 2.5 million to 3 million, defoamer 0.1 part.
[0069] The preparation of the high-density cotton linter pulp is obtained by adding YY-02 penetrating agent for beating and then alkali cooking.
[0070] The alkali-free glass fiber chopped strands are produced by the following method: firstly, the alkali-free glass balls are heated to 1600-1800°C to melt, then the molten alkali-free glass balls are sprayed to obtain glass fibers, and finally the obtained glass fibers are cut to obtain Chopped st...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com